Drill size chart

Number, letter and fractional drills to 1", smallest first
DrillInchmm
#800.01350.343
#790.01450.368
1/640.01560.397
#780.01600.406
#770.01800.457
#760.02000.508
#750.02100.533
#740.02250.572
#730.02400.610
#720.02500.635
#710.02600.660
#700.02800.711
#690.02920.742
#680.03100.787
1/320.03130.794
#670.03200.813
#660.03300.838
#650.03500.889
#640.03600.914
#630.03700.940
#620.03800.965
#610.03900.991
#600.04001.016
#590.04101.041
#580.04201.067
#570.04301.092
#560.04651.181
3/640.04691.191
#550.05201.321
#540.05501.397
#530.05951.511
1/160.06251.588
#520.06351.613
#510.06701.702
#500.07001.778
#490.07301.854
#480.07601.930
5/640.07811.984
#470.07851.994
#460.08102.057
#450.08202.083
#440.08602.184
#430.08902.261
#420.09352.375
3/320.09382.381
#410.09602.438
#400.09802.489
#390.09952.527
#380.10152.578
#370.10402.642
#360.10652.705
7/640.10942.778
#350.11002.794
#340.11102.819
#330.11302.870
#320.11602.946
#310.12003.048
1/80.12503.175
#300.12853.264
#290.13603.454
#280.14053.569
9/640.14063.572
#270.14403.658
#260.14703.734
#250.14953.797
#240.15203.861
#230.15403.912
5/320.15633.969
#220.15703.988
#210.15904.039
#200.16104.089
#190.16604.216
#180.16954.305
11/640.17194.366
#170.17304.394
#160.17704.496
#150.18004.572
#140.18204.623
#130.18504.699
3/160.18754.763
#120.18904.801
#110.19104.851
#100.19354.915
#90.19604.978
#80.19905.055
#70.20105.105
13/640.20315.159
#60.20405.182
#50.20555.220
#40.20905.309
#30.21305.410
7/320.21885.556
#20.22105.613
#10.22805.791
A0.23405.944
15/640.23445.953
B0.23806.045
C0.24206.147
D0.24606.248
E · 1/40.25006.350
F0.25706.528
G0.26106.629
17/640.26566.747
H0.26606.756
I0.27206.909
J0.27707.036
K0.28107.137
9/320.28137.144
L0.29007.366
M0.29507.493
19/640.29697.541
N0.30207.671
5/160.31257.938
O0.31608.026
P0.32308.204
21/640.32818.334
Q0.33208.433
R0.33908.611
11/320.34388.731
S0.34808.839
T0.35809.093
23/640.35949.128
U0.36809.347
3/80.37509.525
V0.37709.576
W0.38609.804
25/640.39069.922
X0.397010.084
Y0.404010.262
13/320.406310.319
Z0.413010.490
27/640.421910.716
7/160.437511.113
29/640.453111.509
15/320.468811.906
31/640.484412.303
1/20.500012.700
33/640.515613.097
17/320.531313.494
35/640.546913.891
9/160.562514.288
37/640.578114.684
19/320.593815.081
39/640.609415.478
5/80.625015.875
41/640.640616.272
21/320.656316.669
43/640.671917.066
11/160.687517.463
45/640.703117.859
23/320.718818.256
47/640.734418.653
3/40.750019.050
49/640.765619.447
25/320.781319.844
51/640.796920.241
13/160.812520.638
53/640.828121.034
27/320.843821.431
55/640.859421.828
7/80.875022.225
57/640.890622.622
29/320.906323.019
59/640.921923.416
15/160.937523.813
61/640.953124.209
31/320.968824.606
63/640.984425.003
11.000025.400