Skip to content
BreakingChips

Steel · ISO P

D2 steel speeds and feeds

Also: SKD11, X153CrMoV12, 1.2601, BD2

Starting points from the same engines as the calculators, with no tool or setup picked. The first number is where to start; the range is what the manufacturer charts allow. Open a calculator for your tool, machine and cut.

Draft data: researched from manufacturer charts, not yet reviewed by a machinist.

Machining notes

Annealed200 HB

Turning

CutSFMFeed, IPRDepth, in
Finishing566390–781173 m/min0.0070.004–0.0100.18 mm/rev0.0220.004–0.0400.6 mm
Medium476328–656145 m/min0.0140.007–0.0200.34 mm/rev0.0850.012–0.1582.2 mm
Roughing447308–617136 m/min0.0170.010–0.0240.43 mm/rev0.1490.060–0.2373.8 mm

For a CVD carbide insert, general stability, 15 min tool life.

Milling, solid carbide end mill

Speed 175 (100–250) SFM · 53 m/min

Chip load per tooth, before chip thinning
Cutter ØIPTmm/tooth
1/8"0.00050.0004–0.00050.011
1/4"0.00120.0010–0.00130.029
1/2"0.00160.0010–0.00210.039
3/4"0.00240.0020–0.00280.061
1"0.00340.0028–0.00400.086

Drilling, Ø1/2" at 3×D

DrillSFMFeed, IPR
HSS5830–880.00700.0053–0.0150
Cobalt6833–880.00740.0060–0.0140
Solid carbide, through-coolant248165–4590.00910.0060–0.0126

Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.

Tapping

Cut tap
58 (40–80) SFM
Form tap
20 (10–35) SFM

Hardened 60 HRC60 HRC

Cuts as ISO H (Hardened)

Turning

Hard turning (ISO H, hardened steel) data isn’t sourced yet.

Milling, solid carbide end mill

Hardened steel (ISO H) milling data isn’t sourced yet.

Drilling, Ø1/2" at 3×D

DrillSFMFeed, IPR
HSSHardened steel needs a carbide drill
CobaltHardened steel needs a carbide drill
Solid carbide, through-coolant10870–1710.00460.0016–0.0070

Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.

Tapping

No sourced tapping speed for hardened steel yet.

Sources