Starting points from the same engines as the calculators, with no tool or setup picked. The first number is where to start; the range is what the manufacturer charts allow. Open a calculator for your tool, machine and cut.

Draft data: researched from manufacturer charts, not yet reviewed by a machinist.

Machining notes

Solution annealed250 HB

Turning

CutSFMFeed, IPRDepth, in
Finishing15678–29348 m/min0.0050.003–0.0070.12 mm/rev0.0220.004–0.0400.6 mm
Medium13166–24640 m/min0.0090.005–0.0130.22 mm/rev0.0850.012–0.1582.2 mm
Roughing12362–23138 m/min0.0110.007–0.0160.28 mm/rev0.1490.060–0.2373.8 mm

For a PVD carbide insert, general stability, 15 min tool life.

Milling, solid carbide end mill

Speed 70 (40–100) SFM · 21 m/min

Chip load per tooth, before chip thinning
Cutter ØIPTmm/tooth
1/8"0.00050.0004–0.00050.011
1/4"0.00110.0010–0.00120.028
1/2"0.00200.051
3/4"0.00300.076
1"0.00350.0030–0.00400.089

Drilling, Ø1/2" at 3×D

DrillSFMFeed, IPR
HSSNot enough published data yet: 2 drill makers give an HSS speed for nickel superalloys, and this site needs 3. Use a cobalt or carbide drill, which 3 or more makers cover.
Cobalt2220–350.00330.0030–0.0035
Solid carbide, through-coolant11870–1650.0030

Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.

Tapping

Cut tap
58 (49–66) SFM
Form tap
No sourced form tapping speed for heat-resistant superalloys yet

Aged350 HB

Turning

CutSFMFeed, IPRDepth, in
Finishing11256–20934 m/min0.0050.003–0.0070.12 mm/rev0.0220.004–0.0400.6 mm
Medium9447–17629 m/min0.0090.005–0.0130.22 mm/rev0.0850.012–0.1582.2 mm
Roughing8844–16527 m/min0.0110.007–0.0160.28 mm/rev0.1490.060–0.2373.8 mm

For a PVD carbide insert, general stability, 15 min tool life.

Milling, solid carbide end mill

Speed 70 (40–100) SFM · 21 m/min

Chip load per tooth, before chip thinning
Cutter ØIPTmm/tooth
1/8"0.00050.0004–0.00050.011
1/4"0.00110.0010–0.00120.028
1/2"0.00200.051
3/4"0.00300.076
1"0.00350.0030–0.00400.089

Drilling, Ø1/2" at 3×D

DrillSFMFeed, IPR
HSSNot enough published data yet: 2 drill makers give an HSS speed for nickel superalloys, and this site needs 3. Use a cobalt or carbide drill, which 3 or more makers cover.
Cobalt2220–350.00330.0030–0.0035
Solid carbide, through-coolant11870–1650.0030

Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.

Tapping

Cut tap
58 (49–66) SFM
Form tap
No sourced form tapping speed for heat-resistant superalloys yet

Sources