M14 × 1.5 tap drill size

For general work, OSG suggests 65–70% of full thread. Harder materials and deep holes want less; the calculator sets it from your material.

Cut tap

12.7 mm

0.5000" · 67% thread

Form tap

13.5 mm

0.5315" · 49% thread

Open M14 × 1.5 in the calculator

Pick your material for its % of thread, tapping RPM and the rigid-tap code.

Thread dimensions

Major Ø
14.000 mm (0.5512")
Pitch
1.5 mm
Pitch Ø (basic)
13.026 mm (0.5128")
Minor Ø (internal, basic)
12.376 mm (0.4873")
Thread depth (internal)
0.812 mm (0.0320")

Basic sizes of the 60° form. Tolerance classes (6H) set the limits around them.

Cut tap drills

For a cutting (fluted or spiral) tap. Every standard drill from 50% to 85% thread; suggested rows are in the 65–70% band.

Cut tap drills for M14 × 1.5
DrillØ inØ mmThread
12.4 mm0.488212.4082%
12.5 mm0.492112.5077%
12.6 mm0.496112.6072%
1/2suggested0.500012.7067%
12.7 mmsuggested0.500012.7067%
12.8 mm0.503912.8062%
12.9 mm0.507912.9056%
13 mm0.511813.0051%

Form tap drills

A form (roll) tap displaces metal instead of cutting it, so it needs a bigger hole. Every standard drill from 50% to 85% thread; suggested rows are in the 65–70% band.

Form tap drills for M14 × 1.5
DrillØ inØ mmThread

3-wire measurement

Best wire size
0.866 mm (0.0341")
Over wires, at basic pitch Ø
14.325 mm (0.5640")

For the external thread (the screw). The best wire touches the flanks at the pitch diameter.