Sheet metal gauge chart

Steel (Manufacturers' Standard Gauge)
GaugeInchmm
30.23916.07
40.22425.69
50.20925.31
60.19434.93
70.17934.56
80.16444.18
90.14953.80
100.13453.42
110.11963.04
120.10462.66
130.08972.28
140.07471.90
150.06731.71
160.05981.52
170.05381.37
180.04781.21
190.04181.06
200.03590.91
210.03290.84
220.02990.76
230.02690.68
240.02390.61
250.02090.53
260.01790.46
270.01640.42
280.01490.38
290.01350.34
300.01200.30
310.01050.27
320.00970.25
330.00900.23
340.00820.21
350.00750.19
360.00670.17
370.00640.16
380.00600.15
Galvanized steel (Galvanized Sheet Gauge)
GaugeInchmm
80.16814.27
90.15323.89
100.13823.51
110.12333.13
120.10842.75
130.09342.37
140.07851.99
150.07101.80
160.06351.61
170.05751.46
180.05161.31
190.04561.16
200.03961.01
210.03660.93
220.03360.85
230.03060.78
240.02760.70
250.02470.63
260.02170.55
270.02020.51
280.01870.47
290.01720.44
300.01570.40
310.01420.36
Stainless steel (U.S. Standard Gauge)
GaugeInchmm
70.18754.76
80.17194.37
90.15633.97
100.14063.57
110.12503.18
120.10942.78
130.09382.38
140.07811.98
150.07031.79
160.06251.59
170.05631.43
180.05001.27
190.04381.11
200.03750.95
210.03440.87
220.03130.79
230.02810.71
240.02500.64
250.02190.56
260.01880.48
270.01720.44
280.01560.40
290.01410.36
300.01250.32
310.01090.28
Aluminum (Brown & Sharpe (AWG))
GaugeInchmm
60.16204.12
70.14433.66
80.12853.26
90.11442.91
100.10192.59
110.09072.30
120.08082.05
130.07201.83
140.06411.63
150.05711.45
160.05081.29
170.04531.15
180.04031.02
190.03590.91
200.03200.81
210.02850.72
220.02530.64
230.02260.57
240.02010.51
250.01790.45
260.01590.40
270.01420.36
280.01260.32
290.01130.29
300.01000.25
310.00890.23