Sheet metal gauge chart
A gauge number is a different thickness in each metal, because each has its own gauge system: 16 gauge is 0.0598" in steel, 0.0635" galvanized, 0.0625" stainless and 0.0508" aluminum. The higher the number, the thinner the sheet. Gauge is a nominal size; measure the stock when the thickness matters.
Printable gauge chart (one page)Bend allowance calculatorEmbed or download (free, CC BY)
Thickness by gauge
Inches, with mm below. Tap a gauge for its page with weights and sources.
| Gauge | Steel | Galvanized steel | Stainless steel | Aluminum |
|---|---|---|---|---|
| 3 ga | 0.2391"6.07 mm | — | — | — |
| 4 ga | 0.2242"5.69 mm | — | — | — |
| 5 ga | 0.2092"5.31 mm | — | — | — |
| 6 ga | 0.1943"4.93 mm | — | — | 0.1620"4.12 mm |
| 7 ga | 0.1793"4.56 mm | — | 0.1875"4.76 mm | 0.1443"3.66 mm |
| 8 ga | 0.1644"4.18 mm | 0.1681"4.27 mm | 0.1719"4.37 mm | 0.1285"3.26 mm |
| 9 ga | 0.1495"3.80 mm | 0.1532"3.89 mm | 0.1563"3.97 mm | 0.1144"2.91 mm |
| 10 ga | 0.1345"3.42 mm | 0.1382"3.51 mm | 0.1406"3.57 mm | 0.1019"2.59 mm |
| 11 ga | 0.1196"3.04 mm | 0.1233"3.13 mm | 0.1250"3.18 mm | 0.0907"2.30 mm |
| 12 ga | 0.1046"2.66 mm | 0.1084"2.75 mm | 0.1094"2.78 mm | 0.0808"2.05 mm |
| 13 ga | 0.0897"2.28 mm | 0.0934"2.37 mm | 0.0938"2.38 mm | 0.0720"1.83 mm |
| 14 ga | 0.0747"1.90 mm | 0.0785"1.99 mm | 0.0781"1.98 mm | 0.0641"1.63 mm |
| 15 ga | 0.0673"1.71 mm | 0.0710"1.80 mm | 0.0703"1.79 mm | 0.0571"1.45 mm |
| 16 ga | 0.0598"1.52 mm | 0.0635"1.61 mm | 0.0625"1.59 mm | 0.0508"1.29 mm |
| 17 ga | 0.0538"1.37 mm | 0.0575"1.46 mm | 0.0563"1.43 mm | 0.0453"1.15 mm |
| 18 ga | 0.0478"1.21 mm | 0.0516"1.31 mm | 0.0500"1.27 mm | 0.0403"1.02 mm |
| 19 ga | 0.0418"1.06 mm | 0.0456"1.16 mm | 0.0438"1.11 mm | 0.0359"0.91 mm |
| 20 ga | 0.0359"0.91 mm | 0.0396"1.01 mm | 0.0375"0.95 mm | 0.0320"0.81 mm |
| 21 ga | 0.0329"0.84 mm | 0.0366"0.93 mm | 0.0344"0.87 mm | 0.0285"0.72 mm |
| 22 ga | 0.0299"0.76 mm | 0.0336"0.85 mm | 0.0313"0.79 mm | 0.0253"0.64 mm |
| 23 ga | 0.0269"0.68 mm | 0.0306"0.78 mm | 0.0281"0.71 mm | 0.0226"0.57 mm |
| 24 ga | 0.0239"0.61 mm | 0.0276"0.70 mm | 0.0250"0.64 mm | 0.0201"0.51 mm |
| 25 ga | 0.0209"0.53 mm | 0.0247"0.63 mm | 0.0219"0.56 mm | 0.0179"0.45 mm |
| 26 ga | 0.0179"0.46 mm | 0.0217"0.55 mm | 0.0188"0.48 mm | 0.0159"0.40 mm |
| 27 ga | 0.0164"0.42 mm | 0.0202"0.51 mm | 0.0172"0.44 mm | 0.0142"0.36 mm |
| 28 ga | 0.0149"0.38 mm | 0.0187"0.47 mm | 0.0156"0.40 mm | 0.0126"0.32 mm |
| 29 ga | 0.0135"0.34 mm | 0.0172"0.44 mm | 0.0141"0.36 mm | 0.0113"0.29 mm |
| 30 ga | 0.0120"0.30 mm | 0.0157"0.40 mm | 0.0125"0.32 mm | 0.0100"0.25 mm |
| 31 ga | 0.0105"0.27 mm | 0.0142"0.36 mm | 0.0109"0.28 mm | 0.0089"0.23 mm |
| 32 ga | 0.0097"0.25 mm | — | — | — |
| 33 ga | 0.0090"0.23 mm | — | — | — |
| 34 ga | 0.0082"0.21 mm | — | — | — |
| 35 ga | 0.0075"0.19 mm | — | — | — |
| 36 ga | 0.0067"0.17 mm | — | — | — |
| 37 ga | 0.0064"0.16 mm | — | — | — |
| 38 ga | 0.0060"0.15 mm | — | — | — |
Weight per square foot
Pounds per square foot, with kg/m² below. Steel and galvanized gauges are defined by weight. Stainless is figured for 304 at0.285 lb/in³ and aluminum for 6061 at 0.0975 lb/in³.
| Gauge | Steel | Galvanized steel | Stainless steel | Aluminum |
|---|---|---|---|---|
| 3 ga | 10.000 lb48.82 kg/m² | — | — | — |
| 4 ga | 9.375 lb45.77 kg/m² | — | — | — |
| 5 ga | 8.750 lb42.72 kg/m² | — | — | — |
| 6 ga | 8.125 lb39.67 kg/m² | — | — | 2.276 lb11.11 kg/m² |
| 7 ga | 7.500 lb36.62 kg/m² | — | 7.695 lb37.57 kg/m² | 2.027 lb9.90 kg/m² |
| 8 ga | 6.875 lb33.57 kg/m² | 7.031 lb34.33 kg/m² | 7.054 lb34.44 kg/m² | 1.805 lb8.81 kg/m² |
| 9 ga | 6.250 lb30.52 kg/m² | 6.406 lb31.28 kg/m² | 6.413 lb31.31 kg/m² | 1.607 lb7.85 kg/m² |
| 10 ga | 5.625 lb27.46 kg/m² | 5.781 lb28.23 kg/m² | 5.771 lb28.18 kg/m² | 1.431 lb6.99 kg/m² |
| 11 ga | 5.000 lb24.41 kg/m² | 5.156 lb25.18 kg/m² | 5.130 lb25.05 kg/m² | 1.275 lb6.22 kg/m² |
| 12 ga | 4.375 lb21.36 kg/m² | 4.531 lb22.12 kg/m² | 4.489 lb21.92 kg/m² | 1.135 lb5.54 kg/m² |
| 13 ga | 3.750 lb18.31 kg/m² | 3.906 lb19.07 kg/m² | 3.848 lb18.79 kg/m² | 1.011 lb4.94 kg/m² |
| 14 ga | 3.125 lb15.26 kg/m² | 3.281 lb16.02 kg/m² | 3.206 lb15.65 kg/m² | 0.900 lb4.39 kg/m² |
| 15 ga | 2.813 lb13.73 kg/m² | 2.969 lb14.49 kg/m² | 2.886 lb14.09 kg/m² | 0.802 lb3.91 kg/m² |
| 16 ga | 2.500 lb12.21 kg/m² | 2.656 lb12.97 kg/m² | 2.565 lb12.52 kg/m² | 0.714 lb3.49 kg/m² |
| 17 ga | 2.250 lb10.99 kg/m² | 2.406 lb11.75 kg/m² | 2.309 lb11.27 kg/m² | 0.636 lb3.10 kg/m² |
| 18 ga | 2.000 lb9.76 kg/m² | 2.156 lb10.53 kg/m² | 2.052 lb10.02 kg/m² | 0.566 lb2.76 kg/m² |
| 19 ga | 1.750 lb8.54 kg/m² | 1.906 lb9.31 kg/m² | 1.796 lb8.77 kg/m² | 0.504 lb2.46 kg/m² |
| 20 ga | 1.500 lb7.32 kg/m² | 1.656 lb8.09 kg/m² | 1.539 lb7.51 kg/m² | 0.449 lb2.19 kg/m² |
| 21 ga | 1.375 lb6.71 kg/m² | 1.531 lb7.48 kg/m² | 1.411 lb6.89 kg/m² | 0.400 lb1.95 kg/m² |
| 22 ga | 1.250 lb6.10 kg/m² | 1.406 lb6.87 kg/m² | 1.283 lb6.26 kg/m² | 0.356 lb1.74 kg/m² |
| 23 ga | 1.125 lb5.49 kg/m² | 1.281 lb6.26 kg/m² | 1.154 lb5.64 kg/m² | 0.317 lb1.55 kg/m² |
| 24 ga | 1.000 lb4.88 kg/m² | 1.156 lb5.65 kg/m² | 1.026 lb5.01 kg/m² | 0.282 lb1.38 kg/m² |
| 25 ga | 0.875 lb4.27 kg/m² | 1.031 lb5.04 kg/m² | 0.898 lb4.38 kg/m² | 0.251 lb1.23 kg/m² |
| 26 ga | 0.750 lb3.66 kg/m² | 0.906 lb4.42 kg/m² | 0.770 lb3.76 kg/m² | 0.224 lb1.09 kg/m² |
| 27 ga | 0.688 lb3.36 kg/m² | 0.844 lb4.12 kg/m² | 0.705 lb3.44 kg/m² | 0.199 lb0.97 kg/m² |
| 28 ga | 0.625 lb3.05 kg/m² | 0.781 lb3.81 kg/m² | 0.641 lb3.13 kg/m² | 0.178 lb0.87 kg/m² |
| 29 ga | 0.563 lb2.75 kg/m² | 0.719 lb3.51 kg/m² | 0.577 lb2.82 kg/m² | 0.158 lb0.77 kg/m² |
| 30 ga | 0.500 lb2.44 kg/m² | 0.656 lb3.20 kg/m² | 0.513 lb2.50 kg/m² | 0.141 lb0.69 kg/m² |
| 31 ga | 0.438 lb2.14 kg/m² | 0.594 lb2.90 kg/m² | 0.449 lb2.19 kg/m² | 0.125 lb0.61 kg/m² |
| 32 ga | 0.406 lb1.98 kg/m² | — | — | — |
| 33 ga | 0.375 lb1.83 kg/m² | — | — | — |
| 34 ga | 0.344 lb1.68 kg/m² | — | — | — |
| 35 ga | 0.313 lb1.53 kg/m² | — | — | — |
| 36 ga | 0.281 lb1.37 kg/m² | — | — | — |
| 37 ga | 0.266 lb1.30 kg/m² | — | — | — |
| 38 ga | 0.250 lb1.22 kg/m² | — | — | — |
Where each column comes from
Show
Each thickness is figured from its gauge system's definition, then checked against 4 published charts. Gauge systems are never mixed: a steel gauge number says nothing about aluminum.
- Steel: Manufacturers' Standard Gauge
The U.S. Standard Gauge weight per square foot divided by 41.82 lb/ft² per inch of thickness. Gauges 3 to 38.
The best-covered gauges:
Checked against 4 published copies
Gauge 3, 4, 5, 6, 29, 31, 32, 33, 34, 35, 36, 37, 38: one chart prints these, so they rest on the definition alone.
- Galvanized steel: Galvanized Sheet Gauge
The U.S. Standard Gauge weight plus 2.5 oz/ft² for the zinc, at 41.82 lb/ft² per inch. Gauges 8 to 31.
The best-covered gauges:
Checked against 4 published copies
Gauge 29, 31: one chart prints these, so they rest on the definition alone.
- Stainless steel: U.S. Standard Gauge
The U.S. Standard Gauge thickness (15 U.S.C. § 206). Gauges 7 to 31.
The best-covered gauges:
Checked against 4 published copies
Gauge 27, 29, 31: one chart prints these, so they rest on the definition alone.
- Aluminum: Brown & Sharpe (AWG)
Brown & Sharpe (American Wire Gauge): 0.005" × 92^((36 − gauge) ÷ 39). Gauges 6 to 31.
The best-covered gauges:
Checked against 4 published copies
Gauge 6, 27, 29, 31: one chart prints these, so they rest on the definition alone.
14 ga: Wikipedia prints 0.063"; the other charts and the definition give 0.0641".
26 ga: Wikipedia prints 0.017"; the other charts and the definition give 0.0159".
Embed or download this chart
Free for classes, shops and wikis under CC BY 4.0: use, print and share it; credit BreakingChips with a link. The embed always shows the current, sourced numbers.
Sources14
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (the weights) (archived Oct 13, 2026)
- Continental Steel, Galvanized sheets: each gauge is 2.5 oz/ft² heavier than the U.S. Standard Gauge (archived Nov 15, 2026)
- 15 U.S.C. § 206, Standard gauge for sheet and plate iron and steel (archived Oct 13, 2026)
- Math: American Wire Gauge (ASTM B258) is defined by 0.005" × 92^((36 − n) / 39), exact by definition (cited, not counted)
- Wikipedia, Sheet metal: gauge table (steel column from Machinery's Handbook, 27th ed.) (archived Oct 21, 2026)
- Metal Supermarkets, Sheet metal gauge chart (archived Sep 30, 2026)
- American Steel & Aluminum, Sheet metal gauge chart (archived Nov 13, 2026)
- Welders Supply, Metal gauge to thickness chart (archived Sep 8, 2026)
- Cleveland-Cliffs, 304/304L stainless product data bulletin (archived Nov 15, 2026)
- Rolled Alloys, 304/304L stainless steel data sheet (archived May 13, 2025)
- Outokumpu, 304/304L data sheet (Imperial, Americas) (archived Nov 2, 2026)
- Protolabs, Aluminum 6061-T651/T6 material data sheet
- Smiths Advanced Metals, 6061 aluminium sheet (archived Nov 16, 2026)
- Alabama Specialty Products, alloy density table (A96061 Al 6061) (archived Oct 14, 2026)