Lathe · Mill
Drilling speeds and feeds calculator
Drill RPM, feed and the right peck cycle for your drill, material and hole depth.
Spindle speed
508RPM
1/2 · .5000" · 12.70 mm
Why: 1018 is soft and sticky, so an HSS drill, starting at 67 SFM.
Cutting speed
67SFM
Window 56 – 81
Median of 5 makers
Feed
.0080IPR
Window .0047 – .0120
Median of 6 makers
- Feed rate
- 4.08 IPM
- Cycle
- G83 full retract
- Program Z
- 2.6502"
- Spindle power
- 1.0 HP
- No machine max RPM set: check 508 RPM against your spindle's top speed, and enter it to cap the spindle.
- Z adds the 118° point (.1502") so the full diameter reaches depth.
- Low carbon: gummy, prone to built-up edge. Use sharp, positive edges and keep speed up.
Fanuc-style · check against your control
G90 G94 G17 S508 M03 G83 Z-2.6502 R.1000 Q.5000 F4.08 G80
A full program for your holes, in Haas, LinuxCNC or Mach4 syntax: peck drilling program.
Why these numbers?
The situation
Low-carbon steel is soft and sticky: it welds to the edge, builds up edge, and makes long chips that don’t break well.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge has to resist welding, and the geometry has to break the chip.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A 118° point adds .1502" to Z, so the full diameter reaches the 2.5" depth.
Geometry: exact by definition
The number
Start at 67 SFM; the makers’ window is 56–81 SFM.
5 sources agree
The number
Feed .0080 IPR; the makers’ window is .0047–.0120 IPR.
6 sources agree
The arithmetic
- HSS drill in low-carbon steel: 95 SFM, the median of 5 makers (they span 80–115).
- Feed at Ø.5000": .01 IPR, the median of 6 makers (they span .0059–.015).
- Hole 5×D deep → speed at 70% (Irwin (Unibit) ×0.7, OSG ×0.8; the lower is used); feed at 80%: only Irwin (Unibit) prints a deep-hole feed reduction, for its own HSS drills (×0.9 at 3–5×D, ×0.8 at 5–6×D). Check your drill maker’s figure.
- Past 3×D: G83 full-retract pecks of 1×D.
Sources
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Redline Tools — Cobalt & HSS drills (p. 340) and coolant-fed solid carbide drills (p. 328): speeds and feeds
- Viking Drill & Tool — Recommended speeds and feeds for HSS drills
- Hertel (MSC) — High speed steel & cobalt drills: speeds and feeds
- YG-1 — HSS & cobalt drill parameters, and Carbide Dream Drills technical information
- Dormer Pramet (Precision Twist Drill) — R10/R15/R18 general purpose jobber drills: AMG speeds and feeds
- Walter Titex — Technical compendium, holemaking 2024: cutting data for HSS drills, A1211 (pp. B74–B75)
- Irwin (Unibit) — Drill reference guide: deep hole drilling parameters
- OSG — NEXUS GDS/GDR drills (Lists 1150, 1650): coefficient for reducing RPM by drilling depth
- Shop rule of thumb: most drills reach 3×D before pecking (makeitfrommetal; machinistguides)
- Sandvik Coromant — Drilling formulas and definitions (net power)
Preview the G-code header
5.0×D, full-diameter depth
Caps the spindle; feed drops with it
What next
How the drilling speeds and feeds calculator works
A 1/2 in HSS drill going 2.5 in deep in annealed 1018 starts at 66.5 SFM: 508 RPM and 4.08 IPM, in a G83 peck cycle to Z-2.6502 so the full diameter reaches depth.
How the drill speeds and feeds calculator works
Maintained by John, former CNC lathe programmer
What it calculates
This drilling speeds and feeds calculator gives the RPM and feed per rev for HSS, cobalt, solid carbide and indexable drills by material and drill size. It slows both down for deep holes, picks the canned cycle (G81, G73 or G83) with a peck depth, and works out the Z depth that puts the full drill diameter at the bottom of the hole.
Type the drill the way it’s marked or called out: a number drill (#7), a letter drill (F), a fraction (13/64) or metric (6.8 mm). It’s for CNC mill and lathe operators and anyone drilling on a manual machine who wants a feed that won’t snap a small drill or rub a big one.
The formulas
Drill RPM
RPM = SFM × 12 ÷ (π × D)
- SFM
- cutting speed at the drill’s outside corner
- D
- drill diameter, inches (metric: Vc × 1000 ÷ (π × D) with D in mm)
Feed rate
IPM = RPM × IPR
- IPR
- feed per revolution for the whole drill, not per lip
Drill point length
L = (D ÷ 2) ÷ tan(point angle ÷ 2)
- L
- length of the cone at the tip
- point angle
- 118° gives 0.300 × D, 135° gives 0.207 × D, 140° gives 0.182 × D
Deep hole reduction
speed × ks(L/D)
feed × kf(L/D)
- L/D
- full-diameter depth ÷ drill diameter
- ks, kf
- the reductions the makers of that drill family print at that depth (carbide makers for carbide, HSS makers for HSS); two makers’ figures are shown and the lower is used
Worked example
A 1/2″ HSS jobber drill, a blind hole 2.5″ deep at full diameter, in annealed 1018 with a 118° point.
- Speed: 95 SFM, the median of five makers (they span 80–115). Feed at 1/2″: .01005 IPR, the median of six makers (they span .0059–.015).
- Depth is 2.5 ÷ 0.5 = 5 × D. The HSS makers’ speed reductions at 5 × D are Irwin 0.7 and OSG 0.8, so the lower, 0.7. Only Irwin prints an HSS feed reduction: 0.8, its own figure for its own drills.
- Speed = 95 × 0.7 = 66.5 SFM, so RPM = 66.5 × 12 ÷ (π × 0.5) = 508 RPM.
- Feed = .01005 × 0.8 = .00804 IPR, so the feed rate = 508 × .00804 = 4.08 IPM.
- Z = 2.5 + 0.300 × 0.5 = 2.650″ to the point.
Past 3 × D with HSS it writes G83 Z-2.6502 R.1 Q.5 F4.08: full-retract pecks of one diameter.
How to use it
What you enter
- Drill
- Number, letter, fraction or metric size. It shows the decimal so you can check it against the drill gauge.
- Material
- The alloy and its condition.
- Drill type and point angle
- HSS, cobalt, solid carbide or indexable, and 118°, 135° or 140°. Carbide can run coolant through the drill.
- Hole
- Depth at full diameter, and blind or through. A through hole adds the point length to clear the bottom.
- Machine max RPM
- Optional. A capped RPM drops the feed rate with it, so the feed per rev stays right.
What you get
- Speed, RPM and feed
- The starting value and the range the makers span, with how many makers it came from.
- Cycle and peck
- G81 for shallow holes, G83 full-retract pecks for HSS and cobalt deeper than 3 × D, G73 chip-break pecks for carbide.
- Z depth
- The programmed depth with the drill point added, so the full diameter reaches the depth on the print.
- Power
- Spindle power from Sandvik’s drilling formula, to check against the machine.
Common mistakes
- Programming the print depth as Z. The print gives full-diameter depth. A 118° point is 0.3 × D long, so a 1/2″ drill needs .150″ more Z.
- Pecking when you don’t need to. The shop rule of thumb is that most drills reach 3 × D without pecking, and through-coolant carbide drills run straight to 8 × D. Pecking a shallow hole only adds cycle time.
- Running a jobber drill too deep. Past 8 × D a standard drill is the wrong tool: use a long-series, parabolic or gun drill.
- Reading feed as per lip. Drill tables give feed per revolution of the whole drill. IPM is RPM × IPR, not RPM × 2 × IPR.
Sources
Speeds and feeds are the median of the drill makers who publish each material and drill class, compared like for like (HSS against HSS, carbide against carbide); a value with fewer than three makers is labeled with who publishes it, or refused. The deep-hole reduction comes only from makers of the same drill family (carbide or HSS); two makers are shown side by side and the lower is used, and where no maker in the set covers a depth (HSS past 6 × D, indexable past 3 × D) the calculator says so instead of borrowing another family’s figure. The 3 × D peck rule is a shop rule of thumb and is labeled as one.
- Redline Tools — Cobalt & HSS drills (p. 340) and coolant-fed solid carbide drills (p. 328): speeds and feeds
- Viking Drill & Tool — Recommended speeds and feeds for HSS drills
- Hertel (MSC) — High speed steel & cobalt drills: speeds and feeds
- YG-1 — HSS & cobalt drill parameters, and Carbide Dream Drills technical information
- Dormer Pramet (Precision Twist Drill) — R10/R15/R18 general purpose jobber drills: AMG speeds and feeds
- Haas Tooling — Cobalt jobber drills; carbide drills, general purpose (plain and TSC) and Inox (TSC): feeds and speeds
- Sutton Tools — Application guide: speeds & feeds, HSS and carbide drills (pp. 484–486)
- Tru-Edge — Solid carbide drills: feeds and speeds
- OSG — Carbide drills, lists 215/220D/200/233, and HY-PRO CARB coolant-through drills: drilling technical
- Amana Tool — 4-facet solid carbide fractional drill recommendations
- Walter Titex — Technical compendium, holemaking 2024: cutting data for solid carbide drills
- Kyocera SGS — Series M080 micro drills, fractional: speed and feed recommendations (catalog p. 109)
- Ingersoll — WinTwist exchangeable-head drills: operating guidelines (NEW-393-2, pp. 9–10)
- Widia — Holemaking master catalog 2017 (inch): VariDrill VDS2_ solid carbide, flood coolant, application data (p. R29)
- Harvey Tool — Miniature drills (series 200xx–204xx, 7036xx, 8100xx–8102xx): speeds & feeds
- Mitsubishi Materials — MZE solid carbide drills, external coolant: recommended cutting conditions (L159)
- Iscar — DR-TWIST indexable drills: machining conditions for large-diameter DR-TWIST drills (57–80 mm)
- MAPAL — ECU-Drill-Steel (SCD360, 361) solid carbide drills: cutting data recommendations
- YG-1 — Technical information for carbide Dream Drills, p. 44: speed and feed by drill length (3×D, 5×D, 8×D)
- Irwin (Unibit) — Drill reference guide: deep hole drilling parameters
- OSG — NEXUS GDS/GDR drills (Lists 1150, 1650): coefficient for reducing RPM by drilling depth
- Mitsubishi Materials — TTD drills: reduction rate of cutting conditions for deep holes
- Sandvik Coromant — Drilling formulas and definitions (net power)
- Shop rule of thumb: most drills reach 3×D before pecking (makeitfrommetal; machinistguides)
Related charts and lessons
- Drill size chartNumber, letter, fraction and metric drills with decimals
- Tap drill chartThe drill for each UNC, UNF and metric thread
- G83 peck drillingFull-retract pecks, Q and R explained
- G73 chip-break drillingHigh-speed pecking for carbide
- G81 drilling cycleThe plain drilling cycle
- Cutting speed chartSFM for drilling by material
- Coming from G-Wizard?Its screens and inputs, mapped to these calculators