Each grade as its own maker prints it: the ISO application range, coating and what it is for, checked against the maker’s catalog. Open a grade for every other maker’s grade rated for the same class, and the reasoning behind it.

When a job runs well, I write down the grade and change one thing at a time after that. Swap the grade and the speed together, and you never know which one fixed it.
Shop note from the maker, a former CNC machinist

Quick numbers

Each maker’s grade for a medium cut, from the insert picker
Steel, medium cutP20Each maker’s grade rated for P20 in its own catalog
Stainless, medium cutM30Each maker’s grade rated for M30 in its own catalog
Cast iron, medium cutK10Each maker’s grade rated for K10 in its own catalog
  • ISCAR IC20K10–K20
  • Kennametal K313K05–K20
  • Mitsubishi MC5105K01–K20
  • Sandvik H13AK10–K30
How many of the 101 listed grades cover each point of the ISO application scale, by group. P: up to 38; M: up to 50; K: up to 31; N: up to 16; S: up to 43; H: up to 11.fewermore gradesPMKNSH011020304050
Where the listed grades sit on the ISO scale; the key shows fewer → more.

Calculators

Fix a problem

Charts

Not listed: Walter (it prints ISO groups, not numbered ranges), and grades no other maker’s verified grade can be compared with. Need a grade for a cut? Use the insert picker.

ISCAR · 31 grades

ISO application ranges, 01 to 50, one row per grade: IC07 M10–M20, N05–N20, S10–S30; IC08 N10–N20; IC20 M10–M25, K10–K20, N05–N25, S05–S20, H05–H15; IC30N P10–P30, M10–M20, H10–H25; IC8250 P10–P35, M05–M20; IC9350 P20–P45, M15–M30; IC6015 M05–M25; IC6025 M15–M35; IC4050 P20–P50, M20–M30, K20–K40; IC635 P30–P50, M20–M40; IC250 P15–P35, M20–M40; IC507 P10–P30, M05–M20, S05–S20, H05–H15; IC807 P10–P30, M05–M20, K10–K30, S05–S20, H05–H15; IC907 P10–P30, M05–M20, K15–K30, N05–N20, S05–S20, H05–H15; IC908 P15–P30, M20–M30, K20–K30, S10–S25, H20–H30; IC1007 P10–P30, M05–M20, K20–K40, S05–S20, H05–H15; IC808 P15–P30, M20–M30, K20–K30, S10–S25, H20–H30; IC1008 P15–P25, M15–M30, K15–K30, S10–S20, H15–H25; IC1028 P20–P50, M20–M40; IC228 P25–P50, M30–M40, K20–K50, N20–N40, S25–S30; IC328 P25–P40, M30–M40, S20–S30; IC354 P20–P40, M10–M30; IC928 P20–P40, M25–M35, S15–S30; IC520 M05–M15, N05–N15, S05–S20; IC830 P20–P40, M25–M35, S15–S30; IC804 S05–S15; IC806 S15–S25; IC903 P10–P20, M15–M25, K10–K20, S10–S20, H10–H20; IC300 P20–P40, M20–M35, S15–S30; IC900 P15–P30, M20–M30, K20–K30, S10–S25, H20–H30; IC882 M25–M40, S20–S30.PMKNSH011020304050IC07IC08IC20IC30NIC8250IC9350IC6015IC6025IC4050IC635IC250IC507IC807IC907IC908IC1007IC808IC1008IC1028IC228IC328IC354IC928IC520IC830IC804IC806IC903IC300IC900IC882
ISCAR’s grades on the ISO application scale, as ISCAR prints them.

ISCAR insert grade chart

ISCAR insert grades
GradeTypeCoatingISO range
IC07uncoated carbideUncoatedM10–M20, N05–N20, S10–S30
IC08uncoated carbideUncoatedN10–N20
IC20uncoated carbideUncoatedM10–M25, K10–K20, N05–N25, S05–S20, H05–H15
IC30NcermetUncoatedP10–P30, M10–M20, H10–H25
IC8250also IC9250CVD-coated carbideCVD, TiCN + Al2O3 + TiNP10–P35, M05–M20
IC9350CVD-coated carbideCVD, TiCN + alpha Al2O3 + TiNP20–P45, M15–M30
IC6015CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M05–M25
IC6025CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M15–M35
IC4050CVD-coated carbideCVD, TiCN + Al2O3 + TiNP20–P50, M20–M30, K20–K40
IC635CVD-coated carbideCVD, TiN + TiC + TiNP30–P50, M20–M40
IC250PVD-coated carbidePVD, TiCN + TiNP15–P35, M20–M40
IC507PVD-coated carbidePVD, TiCN + TiNP10–P30, M05–M20, S05–S20, H05–H15
IC807PVD-coated carbidePVD, TiAlN + TiN (SUMOTEC treated)P10–P30, M05–M20, K10–K30, S05–S20, H05–H15
IC907PVD-coated carbidePVD, TiAlNP10–P30, M05–M20, K15–K30, N05–N20, S05–S20, H05–H15
IC908PVD-coated carbidePVD, TiAlNP15–P30, M20–M30, K20–K30, S10–S25, H20–H30
IC1007PVD-coated carbidePVD, TiAlNP10–P30, M05–M20, K20–K40, S05–S20, H05–H15
IC808PVD-coated carbidePVD, TiAlN/AlTiN + TiN (SUMOTEC)P15–P30, M20–M30, K20–K30, S10–S25, H20–H30
IC1008PVD-coated carbidePVD, AlTiN + TiNP15–P25, M15–M30, K15–K30, S10–S20, H15–H25
IC1028PVD-coated carbidePVD, TiAlN + TiNP20–P50, M20–M40
IC228PVD-coated carbidePVD, AlTiN + TiNP25–P50, M30–M40, K20–K50, N20–N40, S25–S30
IC328PVD-coated carbidePVD, TiCNP25–P40, M30–M40, S20–S30
IC354PVD-coated carbidePVD, TiCNP20–P40, M10–M30
IC928PVD-coated carbidePVD, TiAlNP20–P40, M25–M35, S15–S30
IC520PVD-coated carbidePVD, TiCN + TiNM05–M15, N05–N15, S05–S20
IC830PVD-coated carbidePVD, AlTiN + TiN (SUMOTEC)P20–P40, M25–M35, S15–S30
IC804PVD-coated carbidePVD, AlTiN (SUMOTEC treated)S05–S15
IC806PVD-coated carbidePVD, AlTiN (SUMOTEC treated)S15–S25
IC903PVD-coated carbidePVD, AlTiNP10–P20, M15–M25, K10–K20, S10–S20, H10–H20
IC300PVD-coated carbidePVD, TiCNP20–P40, M20–M35, S15–S30
IC900PVD-coated carbidePVD, AlTiNP15–P30, M20–M30, K20–K30, S10–S25, H20–H30
IC882PVD-coated carbidePVD, AlTiN + TiAlSiN + TiSiNM25–M40, S20–S30

Kennametal · 12 grades

ISO application ranges, 01 to 50, one row per grade: K313 M10–M20, K05–K20, N10–N20, S10–S20; K68 M10–M20, K05–K20, N10–N20, S10–S20; KCS10 P10–P20, M10–M20, K05–K20, N10–N20, S10–S20, H10–H10; KCU10 P10–P20, M10–M20, K05–K20, N10–N20, S10–S20, H10–H10; KCU25 P20–P30, M20–M30, K20–K30, N20–N30, S20–S30; KC5010 P10–P20, M10–M20, K05–K20, N10–N20, S10–S20, H10–H10; KC5025 P20–P30, M20–M30, K20–K30, N20–N30, S20–S30; KC5410 N05–N20; KCP40 P35–P45, M20–M30; KCM15 P20–P25, M10–M20; KCM25 P35–P45, M20–M30; KCM35 P40–P45, M30–M40.PMKNSH011020304050K313K68KCS10KCU10KCU25KC5010KC5025KC5410KCP40KCM15KCM25KCM35
Kennametal’s grades on the ISO application scale, as Kennametal prints them.

Kennametal insert grade chart

Kennametal insert grades
GradeTypeCoatingISO range
K313uncoated carbideUncoatedM10–M20, K05–K20, N10–N20, S10–S20
K68uncoated carbideUncoatedM10–M20, K05–K20, N10–N20, S10–S20
KCS10PVD-coated carbidePVD, AlTiNP10–P20, M10–M20, K05–K20, N10–N20, S10–S20, H10–H10
KCU10PVD-coated carbidePVD, MultilayerP10–P20, M10–M20, K05–K20, N10–N20, S10–S20, H10–H10
KCU25PVD-coated carbidePVD, AlTiNP20–P30, M20–M30, K20–K30, N20–N30, S20–S30
KC5010PVD-coated carbidePVD, AlTiNP10–P20, M10–M20, K05–K20, N10–N20, S10–S20, H10–H10
KC5025PVD-coated carbidePVD, AlTiNP20–P30, M20–M30, K20–K30, N20–N30, S20–S30
KC5410PVD-coated carbidePVD, TiB2N05–N20
KCP40also KCP40BCVD-coated carbideCVD, Thin MTCVD TiCN-Al2O3P35–P45, M20–M30
KCM15also KCM15BCVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3P20–P25, M10–M20
KCM25also KCM25BCVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3P35–P45, M20–M30
KCM35also KCM35BCVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3P40–P45, M30–M40

Mitsubishi · 28 grades

ISO application ranges, 01 to 50, one row per grade: MC7015 M05–M25; US7020 M10–M30; MC7025 M20–M40; US735 M30–M50; US905 S01–S10; VP10RT P10–P30, M10–M30, K10–K30, S05–S25; VP15TF P20–P40, M20–M40, K20–K40; VP20RT M20–M40, K20–K40, S15–S35; VP20MF P20–P40, M20–M40; VP05RT S01–S20; MP9005 S01–S20; MP9015 S05–S25; MP9025 S15–S35; HTi10 K10–K20, N10–N20; MT9005 S01–S20; MT9015 S05–S25; TF15 K20–K20; NX2525 P10–P25, M10–M25, K10–K25; AP25N P05–P25, M05–M25, K05–K25; MS6015 P10–P30; MC6115 P01–P25; MC6125 P10–P35; MP3025 P15–P35; MC5105 K01–K20; MC5115 K05–K25; MC5005 K01–K20; MC5015 K05–K25; UTi20T P25–P40, M25–M40, K20–K35.PMKNS011020304050MC7015US7020MC7025US735US905VP10RTVP15TFVP20RTVP20MFVP05RTMP9005MP9015MP9025HTi10MT9005MT9015TF15NX2525AP25NMS6015MC6115MC6125MP3025MC5105MC5115MC5005MC5015UTi20T
Mitsubishi’s grades on the ISO application scale, as Mitsubishi prints them.

Mitsubishi insert grade chart

Mitsubishi insert grades
GradeTypeCoatingISO range
MC7015CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM05–M25
US7020CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM10–M30
MC7025CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM20–M40
US735CVD-coated carbideCVD, Ti compound, thinM30–M50
US905CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinS01–S10
VP10RTPVD-coated carbidePVDP10–P30, M10–M30, K10–K30, S05–S25
VP15TFPVD-coated carbidePVDP20–P40, M20–M40, K20–K40
VP20RTPVD-coated carbidePVDM20–M40, K20–K40, S15–S35
VP20MFPVD-coated carbidePVDP20–P40, M20–M40
VP05RTPVD-coated carbidePVDS01–S20
MP9005PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS01–S20
MP9015PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS05–S25
MP9025PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS15–S35
HTi10uncoated carbideUncoatedK10–K20, N10–N20
MT9005uncoated carbideUncoatedS01–S20
MT9015also RT9010uncoated carbideUncoatedS05–S25
TF15micro-grain carbideUncoatedK20–K20
NX2525cermetUncoatedP10–P25, M10–M25, K10–K25
AP25Nalso VP25NcermetPVDP05–P25, M05–M25, K05–K25
MS6015PVD-coated carbidePVDP10–P30
MC6115CVD-coated carbideCVD, Accumulated TiCN-Al2O3-Ti compound, thickP01–P25
MC6125CVD-coated carbideCVD, Accumulated TiCN-Al2O3-Ti compound, thickP10–P35
MP3025cermetPVD, Ti compoundP15–P35
MC5105CVD-coated carbideCVD, TiCN-Al2O3, thickK01–K20
MC5115CVD-coated carbideCVD, TiCN-Al2O3, thickK05–K25
MC5005CVD-coated carbideCVDK01–K20
MC5015CVD-coated carbideCVDK05–K25
UTi20Tuncoated carbideUncoatedP25–P40, M25–M40, K20–K35

Sandvik · 15 grades

ISO application ranges, 01 to 50, one row per grade: GC4305 P01–P15; GC4315 P01–P30; GC4325 P10–P40; GC4335 P25–P45; GC2015 M05–M25; GC2025 M15–M35; GC2220 M15–M30; GC2035 M25–M40; GC1115 M05–M25, S15–S25; GC1125 M10–M30, S20–S30; GC1105 S05–S20; S05F S05–S15; H13A K10–K30, N05–N25, S10–S30; H10 N01–N25; GC1525 P05–P25.PMKNS011020304050GC4305GC4315GC4325GC4335GC2015GC2025GC2220GC2035GC1115GC1125GC1105S05FH13AH10GC1525
Sandvik’s grades on the ISO application scale, as Sandvik prints them.

Sandvik insert grade chart

Sandvik insert grades
GradeTypeCoatingISO range
GC4305CVD-coated carbideCVDP01–P15
GC4315CVD-coated carbideCVDP01–P30
GC4325CVD-coated carbideCVDP10–P40
GC4335CVD-coated carbideCVDP25–P45
GC2015CVD-coated carbideCVDM05–M25
GC2025CVD-coated carbideCVDM15–M35
GC2220CVD-coated carbideCoated (process not printed)M15–M30
GC2035PVD-coated carbidePVDM25–M40
GC1115PVD-coated carbidePVDM05–M25, S15–S25
GC1125PVD-coated carbidePVDM10–M30, S20–S30
GC1105PVD-coated carbidePVDS05–S20
S05FCVD-coated carbideCVDS05–S15
H13Auncoated carbideUncoatedK10–K30, N05–N25, S10–S30
H10uncoated carbideUncoatedN01–N25
GC1525cermetPVDP05–P25

Seco · 15 grades

ISO application ranges, 01 to 50, one row per grade: TH1000 S01–S10, H05–H15; TS2000 M01–M10, S05–S20; TS2050 S05–S15; TS2500 S10–S20; CP200 M01–M10, S10–S20; CP500 M10–M30; CP600 M20–M40; TS0501 S01–S05; TM1501 M10–M20; TM2501 M20–M25; TM3501 M25–M35; HX S10–S25; 883 S10–S30; 890 S10–S20; TP1030 P10–P20.PMSH011020304050TH1000TS2000TS2050TS2500CP200CP500CP600TS0501TM1501TM2501TM3501HX883890TP1030
Seco’s grades on the ISO application scale, as Seco prints them.

Seco insert grade chart

Seco insert grades
GradeTypeCoatingISO range
TH1000PVD-coated carbidePVD, Ti-Al-Si-N nanolaminateS01–S10, H05–H15
TS2000PVD-coated carbidePVD, (Ti,Al)N + TiNM01–M10, S05–S20
TS2050PVD-coated carbidePVD, Ti-Al-Si-N nanolaminateS05–S15
TS2500PVD-coated carbidePVD, (Ti,Al)N + TiNS10–S20
CP200PVD-coated carbidePVD, (Ti,Al)N + TiNM01–M10, S10–S20
CP500PVD-coated carbidePVD, (Ti,Al)N + TiNM10–M30
CP600PVD-coated carbidePVD, (Ti,Al)N + TiNM20–M40
TS0501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerS01–S05
TM1501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerM10–M20
TM2501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerM20–M25
TM3501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerM25–M35
HXuncoated carbideUncoatedS10–S25
883micro-grain carbideUncoatedS10–S30
890micro-grain carbideUncoatedS10–S20
TP1030cermetPVD, Ti-Al-Si-N nanolaminateP10–P20