Lathe
Speeds, feeds, threading and tapers for the lathe, with fixes for chips and chatter.
Before I trust a new tool, I take a skim cut, mic the part and set the wear offset from the mic, not from the presetter.
Quick numbers
Turning speed for a coated carbide insert, medium cut (aluminum: uncoated)Carbon steel650 SFMMedian of 6 makers. Middle half 623–860; all 440–1,312
304 and 316 stainless551 SFMMedian of 6 makers. Middle half 492–623; all 295–787
Gray cast iron1,041 SFMMedian of 6 makers. Middle half 830–1,320; all 492–2,297
Aluminum1,645 SFMMedian of 4 makers. Middle half 1,315–1,891; all 328–3,937
Calculators
- Turning speeds and feeds calculatorMaterial, insert and setup to speed, feed, DOC, RPM and G-code.
- Knurling calculatorThe blank Ø that tracks, form growth, tooth depth, speeds and feeds.
- Taper calculatorTaper per foot, included angle and compound setting; small end from an angle; tailstock offset.
- Surface finish calculatorFeed and nose radius to Ra, or an Ra callout to the max feed; ball end mill cusp height.
- Change gear calculatorThe change gears (A, B, C, D) for any TPI or metric pitch from your leadscrew and the gears you have: exact trains first, then the closest.
- Thread dial calculatorWhich line to close the half nut on for any TPI or metric pitch, worked from your leadscrew, dial gear and dial lines.
- Single-point threading calculatorThread depth, compound setting, passes and infeed, the thread dial for your lathe, a G76 line for Fanuc or Haas, and the wire check.
- HSS lathe tool grindingThe rake, relief and cutting-edge angles to grind a high-speed steel lathe tool for your material, with the tool drawn and the grinding order.
Fix a problem
- Chatter and vibrationA loud whine or buzz, and a wavy pattern on the part. Worst in boring and on long, thin parts.
- Long, stringy chipsChips come off in long ribbons or bird’s nests that wrap the part, the tool or the chuck.
- Rough, torn or hairy finishThe finish misses the print: torn, smeared or scratched, or a feed pattern too coarse to pass.
- Built-up edgeWorkpiece material welds onto the edge, then tears off, taking coating with it. Common in soft steel, stainless and aluminum.
- Inserts wear out fastEven wear land on the flank grows quickly; size drifts and finish fades well before the expected life.
- Chips too short, hard or hammeredTiny chips that fly, weld together or hammer the edge; the cut sounds harsh and inserts chip early.
Charts
Guides
Show 7 guides
- Knurling that tracksWhy a knurl double tracks, how to find the diameter that doesn’t, and how form and cut knurling differ.
- Three ways to turn a taperCompound rest, offset tailstock or taper attachment: which one fits the taper, and the setting each one needs.
- Steady rest vs follower restWhich rest for long or thin work: the steady rest fixed on the bed, or the follower rest riding the carriage behind the tool.
- Buying a used lathe or millWhat to check on a used lathe or knee mill before you pay: ways, spindle, slides, drive, power, tooling and the machine’s age.
- 3-jaw vs 4-jaw vs Set-Tru chucksWhat each lathe chuck is for, why a 3-jaw never runs dead true, how a Set-Tru fixes that, and when a collet beats them all.
- Speeds and feedsCutting speed, RPM, feed per rev and chip load: what each one is, and what each one changes.
- Indicating work in a 4-jaw chuckCentring a part to tenths in a 4-jaw: read opposite jaws, split the difference, and set an offset on purpose.
Sources
Sources6
- Kennametal — Turning inserts, carbide: RP, MP, FP and MS geometries, cutting speed (SFM) ranges and starting feeds (archived Nov 15, 2026)
- Mitsubishi Materials USA — Optimum Grades and Chip Breakers for External Turning (archived Aug 3, 2024)
- Kyocera — Recommended cutting conditions, external turning (negative inserts), catalog pp. D46–D47 (archived Nov 13, 2026)
- Tungaloy — General catalog 2023–2024, inserts: chipbreaker guide, standard cutting conditions and selection system (pp. B004–B013) (archived Jan 21, 2025)
- Sumitomo Electric — General catalogue 2018–2019, insert selection: recommended cutting conditions (pp. A5–A12) (archived Nov 16, 2026)
- Korloy — Turning: recommended chip breaker for workpiece, cutting speeds and feeds (pp. B4–B11) (archived Aug 19, 2022)