Home › Materials › Cutting speed chart Steel Steel: starting cutting speeds in SFM Material, condition Turning, carbide End mill, carbide Drill, HSS Drill, carbide Tap, cut 1018 , Hot rolled / annealed 975 491 95 383 63 1020 , Hot rolled / annealed 975 491 95 383 63 1045 , Annealed / normalized 684 414 74 362 58 1045 , Quenched & tempered 619 374 74 362 58 12L14 , Cold drawn 591 357 74 362 58 1144 , Cold drawn / stress relieved 591 357 74 362 58 4140 , Annealed 542 328 74 362 55 4140 , Quenched & tempered (pre-hard, ~28–32 HRC) 394 238 39 251 55 4140 , Hardened 50 HRC 418 — — 108 — 4340 , Annealed 542 328 74 362 55 4340 , Quenched & tempered 394 238 39 251 55 4340 , Hardened 50 HRC 418 — — 108 — 8620 , Annealed / as rolled 743 449 74 362 55 52100 , Spheroidize annealed 500 302 74 362 55 52100 , Hardened 60 HRC 584 — — 108 — A2 , Annealed 700 200 58 248 55 A2 , Hardened 60 HRC 584 — — 108 — D2 , Annealed 700 200 58 248 55 D2 , Hardened 60 HRC 584 — — 108 — H13 , Annealed 700 200 58 248 55 H13 , Hardened & tempered (pre-hard) 368 105 58 248 55 H13 , Hardened 50 HRC 418 — — 108 — O1 , Annealed 500 302 74 362 55 O1 , Hardened 60 HRC 584 — — 108 —
Stainless Stainless: starting cutting speeds in SFM Material, condition Turning, carbide End mill, carbide Drill, HSS Drill, carbide Tap, cut 303 , Annealed 551 293 33 176 30 304 , Annealed 551 293 33 176 30 316 , Annealed 551 293 33 176 30 410 , Annealed 640 210 45 202 30 410 , Hardened & tempered 388 127 45 202 30 416 , Annealed 640 210 45 202 30 420 , Annealed 640 210 45 202 30 420 , Hardened & tempered 388 127 45 202 30 17-4 PH , Condition A (solution annealed) 412 135 45 202 30 17-4 PH , H1150 448 147 20 183 30 17-4 PH , H900 320 105 20 183 30 2205 Duplex , Solution annealed 394 — — — 30
Cast iron Cast iron: starting cutting speeds in SFM Material, condition Turning, carbide End mill, carbide Drill, HSS Drill, carbide Tap, cut Gray iron, Class 30 , As cast 935 359 88 436 48 Ductile iron, 65-45-12 , As cast (ferritic/pearlitic) 853 378 64 329 32 Ductile iron, 80-55-06 , As cast (pearlitic) 692 378 64 329 32
Non-ferrous Non-ferrous: starting cutting speeds in SFM Material, condition Turning, carbide End mill, carbide Drill, HSS Drill, carbide Tap, cut 6061 , T6 1,645 600 250 651 80 6061 , O (annealed) 1,645 600 250 651 80 7075 , T6 / T651 1,645 600 250 651 80 2024 , T3 / T351 1,645 600 250 651 80 A356 cast aluminum , T6 1,645 600 250 651 80 360 brass , Half hard 1,315 400 139 513 72 932 bearing bronze , As cast 1,315 400 139 513 72 C110 copper , Half hard — 400 139 513 72
Superalloys & titanium Superalloys & titanium: starting cutting speeds in SFM Material, condition Turning, carbide End mill, carbide Drill, HSS Drill, carbide Tap, cut Ti-6Al-4V , Annealed 189 170 39 127 29 CP titanium, Grade 2 , Annealed 283 170 39 127 29 Inconel 718 , Solution annealed 184 70 15 118 16 Inconel 718 , Aged 131 70 15 118 16 Inconel 625 , Annealed 184 70 15 118 16 Hastelloy X , Solution annealed 184 70 15 118 16
Embed or download this chart Free for classes, shops and wikis under CC BY 4.0 : use, print and share it; credit BreakingChips with a link. The embed always shows the current, sourced numbers.
SFM × 0.3048 = m/min. Turning is a medium cut with a coated carbide insert; drills are Ø1/2" at 3×D.