Press fit calculator

Contact pressure, press force, holding torque and shrink temperature for an interference fit.

Press force

59.4kN

Interference
1 µm to 42 µm
Pressure
1.5 MPa to 63.0 MPa
Hub bore stress
up to 105.0 MPa
Holds (loosest)
35.3 N·m
Shrink fit
heat the hub 70 °C, or cool the shaft 70 °C
Material stiffness:

Only two makers publish this: Engineering ToolBox and AZoM

Why: Press it on with up to 59.4 kN; at its loosest it is sure to hold 35.3 N·m.

Units
Interference from

The shaft and bore size

H7/p6 press, H7/s6 heavy press

Your own value: we have not found two published tables that agree

Added to the heating temperature

Why these numbers?
  1. The situation

    H7/p6 at 50 mm interferes by 1 µm to 42 µm on the diameter.

    From your input: the fit you picked (ISO 286 limits)

  2. What that means

    Pressed together, the hub stretches and the shaft squeezes until both push back with the same pressure. A stiffer material and a thicker hub give more pressure for the same interference.

    Geometry: exact by definition

  3. What that means

    Carbon or alloy steel: E 200 GPa, from Engineering ToolBox and AZoM.

    Two sources: Engineering ToolBox and AZoM

  4. So

    Check both ends of the tolerance: the loosest parts (1.5 MPa) set the torque it is sure to carry; the tightest (63.0 MPa) set the press force and stress the hub bore to 105.0 MPa.

    Geometry: exact by definition

  5. What that means

    Friction μ = 0.15: press force = π × d × L × p × μ, torque = force × d ÷ 2.

    From your input: your friction coefficient

  6. The number

    For a shrink fit, carbon or alloy steel grows 11.9 µm per metre per °C, so a Ø50 mm bore needs 70 °C more than the shaft to open the tightest parts.

    Geometry: exact by definition

How we source these numbers

A press fit in half section: a hub 100 mm across, 40 mm long, on a 50 mm shaft, its bore smaller than the shaft by the interference, 1 µm to 42 µm.hub OD 100 mmshaft Ø 50 mmhub length 40 mminterference 1 µm to 42 µm
The hub on the shaft in half section. Not to scale; the interference drawn far larger than true.

What next

What limits give this fit?Hole and shaft limits for an ISO fit like H7/g6, and how tightly they mate.
Where do the holes on this bolt circle go?X and Y for every hole on a bolt circle, plus a G81 drilling program.
What are the missing sides and angles?A right triangle's missing sides and angles from two sides, or a side and angle.
How the press fit calculator works

A steel hub 100 mm across and 40 mm long on a 50 mm steel shaft at H7/p6 takes up to 59.4 kN to press on, holds as little as 35.3 N·m at the loose end of the fit, and shrinks on with the hub 70 °C hotter than the shaft.

Press fit and shrink fit: pressure, press force and heating temperature

Maintained by John, former CNC lathe programmer

What it calculates

This press fit calculator takes an interference fit, either an ISO fit such as H7/p6 at a size or the least and most interference you measured, plus the hub and shaft sizes and materials. It gives the contact pressure, the stress in the hub bore, the force to press it together, the torque it will hold, and how hot to heat the hub (or how cold to chill the shaft) to slip it together as a shrink fit.

It works both ends of the tolerance, because they answer different questions: the tightest parts decide whether your press is big enough and whether the hub survives, and the loosest parts decide what the joint is sure to carry.

The formulas

Contact pressure (Lamé, thick-walled cylinders)

p = δ ÷ ( d/Eh × [(D² + d²)/(D² − d²) + νh] + d/Es × [(d² + di²)/(d² − di²) − νs] )

δ
diametral interference: shaft diameter minus bore diameter
d, D, di
fit diameter, hub outside diameter, shaft bore (0 if solid)
E, ν
elastic modulus and Poisson’s ratio of the hub (h) and shaft (s)

Same material and a solid shaft: p = E × δ × (D² − d²) ÷ (2 × d × D²).

Hub bore stress

σ = p × (D² + d²) ÷ (D² − d²)

σ
hoop (tangential) stress at the bore, the highest in the hub

Press force and torque

F = π × d × L × p × μ

T = F × d ÷ 2

L
engagement length
μ
friction coefficient between the parts

Shrink fit temperature

ΔT = (δmax + c) ÷ (α × d)

α
linear expansion coefficient of the part being heated or cooled
c
slip clearance wanted at assembly

Worked example

A steel hub, 100 mm OD and 40 mm long, on a solid 50 mm steel shaft, H7/p6 (1 to 42 µm interference), μ = 0.15.

  1. Tightest: p = 200,000 × 0.042 ÷ (2 × 50) × (100² − 50²) ÷ 100² = 84 × 0.75 = 63.0 MPa.
  2. Hub bore stress = 63.0 × (10,000 + 2,500) ÷ (10,000 − 2,500) = 105.0 MPa.
  3. Press force = π × 50 × 40 × 63.0 × 0.15 = 59,376 N, about 59.4 kN (6.7 US tons).
  4. Loosest: p = 200,000 × 0.001 ÷ 100 × 0.75 = 1.5 MPa; torque = π × 50 × 40 × 1.5 × 0.15 × 25 = 35,343 N·mm = 35.3 N·m.
  5. Shrink: ΔT = 0.042 ÷ (0.0000119 × 50) = 70 °C hotter than the shaft, before any slip clearance.

A 10-ton press does it, but the same fit at its loose end holds only 35 N·m: key it, or pick a tighter fit if it must carry torque.

How to use it

What you enter

Interference
An ISO fit and size (the fit’s limits come from the fits calculator), or the least and most interference you measured, on the diameter.
Hub and shaft
Hub outside diameter, engagement length, and the shaft bore if it is hollow.
Materials
Steel, 304 stainless, 6061 aluminum, C360 brass or C932 bronze for each part.
Friction coefficient
Needed for the force and torque. Enter your own value; it depends on finish, lubrication and how the parts go together.

What you get

Press force
At the tightest parts: what the press has to push.
Contact pressure and hub stress
At both ends of the tolerance; compare the hub stress with the hub material’s yield strength.
Torque
At the loosest parts: what the joint is sure to hold on friction.
Shrink fit temperature
How much hotter the hub, or colder the shaft, has to be to open the tightest parts.

Common mistakes

  • Checking only the nominal. The pressure runs from the loosest to the tightest parts, here 1.5 to 63 MPa. Size the press on the tightest and the torque on the loosest.
  • Radial versus diametral interference. The formula uses the difference in diameters. Half of it, the radial interference, gives half the pressure.
  • A thin hub. As the hub OD approaches the bore, the hub stretches more and its bore stress climbs. Check the stress against the hub’s yield strength.
  • Overheating a hardened hub. Heating past the hub’s tempering temperature softens it. If the temperature is too high, chill the shaft instead or use a lighter fit.

Sources

The formulas are Lamé’s thick-walled cylinder equations, geometry cited rather than counted. Each material’s E, ν and α is the midpoint of two publishers, both named. No friction value is supplied: we have not found two published press-fit friction tables that agree, so it is your input. The edge of the hub carries more pressure than Lamé predicts; this is a starting value, not a design check.