Lathe

Turning speeds and feeds calculator

Lathe SFM, feed and depth of cut for your material and insert, with the RPM.

Units
Add your machine

Your cut

Spindle speed at Ø2"

1,035RPM

Starting point · from published maker charts

Why: 4140 runs the edge hot, so a CVD grade, starting at 542 SFM.

Cutting speed

542SFM

Window 367 – 1,093

Median of 6 makers

Feed

.0135IPR

Window .0040 – .0200

Median of 5 makers

Depth of cut

.098in

Window .012 – .197

OD turning a Ø2 in bar: depth of cut .098 in, feed / rev .0135 in.Ø2 infeed / rev .0135 ininserttoolholderdepth of cut .098 inworkchuck
Side view of the bar in the chuck. Depth of cut drawn about 1.2× its true size. The work’s length is not to scale.
RPM window
700 – 2,088
Grade
CVD-coated carbide
Spindle power
10.0 HP
  • No machine max RPM set: check 1,035 RPM against your spindle's top speed, and enter it to cap the spindle.
  • No G50 line in the header until you enter your machine’s max RPM: G50 clamps G96 there as the diameter comes down.

Fanuc-style · check against your control

G96 S542 M03 (SFM)
G99 (FEED PER REV)
G01 F.0135
Why these numbers?
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.

    Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]

  3. The number

    Start at 542 SFM; the makers’ window is 367–1,093 SFM.

    6 sources agree

The arithmetic

  1. CVD-coated carbide in carbon & low-alloy steel: 650 SFM, the median of 6 makers (they span 440–1312) [198 m/min] at 200 HB, medium cut, general setup, 15 min tool life.
  2. Hardness 240 HB vs 200 HB reference → ×0.83.
  3. Feed for a medium cut in steel: .0135 IPR, the median of 5 makers (they span .004–.02); depth of cut likewise.

Sources

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Sandvik Coromant — Cutting tool materials
  4. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining)
  5. Kennametal — Turning inserts, carbide: RP, MP, FP and MS geometries, cutting speed (SFM) ranges and starting feeds
  6. Mitsubishi Materials USA — Optimum Grades and Chip Breakers for External Turning
  7. Kyocera — Recommended cutting conditions, external turning (negative inserts), catalog pp. D46–D47
  8. Tungaloy — General catalog 2023–2024, inserts: chipbreaker guide, standard cutting conditions and selection system (pp. B004–B013)
  9. Sumitomo Electric — General catalogue 2018–2019, insert selection: recommended cutting conditions (pp. A5–A12)
  10. Korloy — Turning: recommended chip breaker for workpiece, cutting speeds and feeds (pp. B4–B11)

How we source these numbers

Preview the G-code header

Tap an answer to change it.

On a mill instead? Milling speeds and feeds for end mills and face mills.

What next

Which tap drill for this thread?Tap drill size for any thread, cut or form tap, by percent of thread.
What finish will this feed leave?The Ra a feed and nose radius leave, or the feed an Ra callout allows.
What RPM and feed for this drill?Drill RPM, feed and the right peck cycle for your drill, material and hole depth.
How the turning speeds and feeds calculator works

Annealed 4140 starts at 542 SFM and 0.0135 IPR in a medium cut with a CVD-coated insert (the median of 6 makers, scaled for its hardness): 1,035 RPM on a 2 in bar.

How the lathe speeds and feeds calculator works

Maintained by John, former CNC lathe programmer

What it calculates

This turning speeds and feeds calculator gives a starting cutting speed (SFM or m/min), feed per rev and depth of cut for OD turning, facing and boring with a carbide or cermet insert, then turns them into the RPM, the G96 constant surface speed block, clamped at your max RPM, and the spindle power the cut will pull.

It is built for the person standing at the lathe: an apprentice who needs a reliable first number, or a setup machinist checking a program before the first part. It asks the questions in the order you think about the job and shows the reason and the source behind each number.

The formulas

Spindle speed from cutting speed

RPM = SFM × 12 ÷ (π × D)

RPM = Vc × 1000 ÷ (π × D)

SFM
surface feet per minute (inch)
Vc
cutting speed, m/min (metric)
D
the workpiece diameter being cut, in inches or mm (not the tool)

Starting cutting speed

Vc = makers’ median × hardness × cutting area × stability × tool life

makers’ median
the median of the insert makers’ published speeds for that material family and grade class
hardness
reference HB ÷ your HB, held between 0.5 and 1.5
cutting area
finish 1.20, light 1.11, medium 1.00, rough 0.91, heavy 0.84
stability
rigid 1.125, average 1.00, interrupted 0.835
tool life
(15 ÷ T)^0.25 for a tool life of T minutes

Each factor is the makers’ median, or a named pair where only two print one.

Theoretical finish from feed and nose radius

Rz = f² ÷ 8r

Ra ≈ f² ÷ 32r

f
feed per revolution
r
insert nose radius, same unit as f

Cutting force and power (Kienzle)

h = f × sin κr

kc = kc1.1 × h^−mc

Pc = kc × ap × f × Vc ÷ 60,000

h
chip thickness, mm
κr
entering angle (90° for a square shoulder)
kc1.1, mc
the material’s specific cutting force at 1 mm chip, and how fast it rises as the chip thins
ap
depth of cut, mm
Pc
cutting power, kW; spindle power divides by a drive efficiency of 0.8

Worked example

A 2.000″ bar of carbon steel at 200 HB, a medium cut in a general setup with a CVD-coated insert and a 1/32″ (.03125″) nose radius. The makers’ median speed is 650 SFM, every factor is 1.00 at these settings, and the medium-cut feed starts at .0135 IPR.

  1. RPM = 650 × 12 ÷ (π × 2.000) = 7,800 ÷ 6.283 = 1,241 RPM.
  2. Feed rate = .0135 IPR × 1,241 RPM = 16.8 in/min along Z.
  3. Theoretical Ra = .0135² ÷ (32 × .03125) = .000182 ÷ 1.000 = 182 µin, about 4.6 µm.

Program G96 S650 with a G50 clamp under your spindle’s top speed. If the print calls for 125 µin, the feed for that Ra on this nose is √(32 × .03125 × .000125) = .0112 IPR.

How to use it

What you enter

Material and condition
Pick the alloy and its heat treat or hardness. Hardness changes the speed, so annealed and pre-hardened 4140 give different answers.
Operation
Finish, light, medium, rough or heavy. Each has its own feed and depth window from the makers.
Insert and grade
The insert shape and nose radius cap the depth of cut and the feed; the grade class (CVD, PVD, cermet, uncoated) picks which makers’ speed table is used.
Setup and machine
How stable the setup is, plus your spindle’s max RPM and power if you have them, so the answer can warn before you stall or overspeed.

What you get

Cutting speed, feed and depth of cut
The starting value with the range the makers span. Start in the middle and adjust by the chips and the finish.
RPM and G96 / G50
RPM at your diameter, and the constant surface speed block with a clamp that keeps the spindle under its limit when facing toward center.
Finish and power
The geometric Ra from feed and nose radius, and the spindle power and torque against your machine.

Common mistakes

  • Using the tool diameter. On a lathe D is the part diameter where the insert is cutting. As you turn down a bar the RPM has to rise to hold the same SFM, which is what G96 does for you.
  • Facing to center with no clamp. Constant surface speed asks for infinite RPM at X0. Set G50 S to the machine’s or chuck’s rated maximum RPM before G96.
  • Depth of cut smaller than the nose radius. Sandvik recommends a depth of cut close to or bigger than the nose radius; below it the chip won’t break well and the insert rubs.
  • Feeding too hard for the nose. Each nose radius has a top feed before the corner is at risk. The calculator caps the feed at Sandvik’s recommended maximum for the radius you pick.

Sources

Cutting speeds are the median of the insert makers’ published values for each material family and grade class; with fewer than two the calculator says there isn’t enough published data. Feed and depth windows are the makers’ medians by cutting area. RPM, finish and power are math.

How we pick and check sources