Printable cutting speed chart
Back to the full chart
One page on Letter or A4. To save a PDF, pick "Save as PDF" in the print dialog.
| Material, condition | Turning, carbide | End mill, carbide | Drill, HSS | Drill, carbide | Tap, cut |
|---|---|---|---|---|---|
| 1018, Hot rolled / annealed | 975 | 491 | 95 | 383 | 63 |
| 1020, Hot rolled / annealed | 975 | 491 | 95 | 383 | 63 |
| 1045, Annealed / normalized | 684 | 414 | 74 | 362 | 58 |
| 1045, Quenched & tempered | 619 | 374 | 74 | 362 | 58 |
| 12L14, Cold drawn | 591 | 357 | 74 | 362 | 58 |
| 1144, Cold drawn / stress relieved | 591 | 357 | 74 | 362 | 58 |
| 4140, Annealed | 542 | 328 | 74 | 362 | 55 |
| 4140, Quenched & tempered (pre-hard, ~28–32 HRC) | 394 | 238 | 39 | 251 | 55 |
| 4140, Hardened 50 HRC | 418 | — | — | 108 | — |
| 4340, Annealed | 542 | 328 | 74 | 362 | 55 |
| 4340, Quenched & tempered | 394 | 238 | 39 | 251 | 55 |
| 4340, Hardened 50 HRC | 418 | — | — | 108 | — |
| 8620, Annealed / as rolled | 743 | 449 | 74 | 362 | 55 |
| 52100, Spheroidize annealed | 500 | 302 | 74 | 362 | 55 |
| 52100, Hardened 60 HRC | 584 | — | — | 108 | — |
| A2, Annealed | 700 | 200 | 58 | 248 | 55 |
| A2, Hardened 60 HRC | 584 | — | — | 108 | — |
| D2, Annealed | 700 | 200 | 58 | 248 | 55 |
| D2, Hardened 60 HRC | 584 | — | — | 108 | — |
| H13, Annealed | 700 | 200 | 58 | 248 | 55 |
| H13, Hardened & tempered (pre-hard) | 368 | 105 | 58 | 248 | 55 |
| H13, Hardened 50 HRC | 418 | — | — | 108 | — |
| O1, Annealed | 500 | 302 | 74 | 362 | 55 |
| O1, Hardened 60 HRC | 584 | — | — | 108 | — |
| 303, Annealed | 551 | 293 | 33 | 176 | 30 |
| 304, Annealed | 551 | 293 | 33 | 176 | 30 |
| 316, Annealed | 551 | 293 | 33 | 176 | 30 |
| 410, Annealed | 640 | 210 | 45 | 202 | 30 |
| 410, Hardened & tempered | 388 | 127 | 45 | 202 | 30 |
| 416, Annealed | 640 | 210 | 45 | 202 | 30 |
| 420, Annealed | 640 | 210 | 45 | 202 | 30 |
| 420, Hardened & tempered | 388 | 127 | 45 | 202 | 30 |
| 17-4 PH, Condition A (solution annealed) | 412 | 135 | 45 | 202 | 30 |
| 17-4 PH, H1150 | 448 | 147 | 20 | 183 | 30 |
| 17-4 PH, H900 | 320 | 105 | 20 | 183 | 30 |
| 2205 Duplex, Solution annealed | 394 | — | — | — | 30 |
| Gray iron, Class 30, As cast | 935 | 359 | 88 | 436 | 48 |
| Ductile iron, 65-45-12, As cast (ferritic/pearlitic) | 853 | 378 | 64 | 329 | 32 |
| Ductile iron, 80-55-06, As cast (pearlitic) | 692 | 378 | 64 | 329 | 32 |
| 6061, T6 | 1,645 | 600 | 250 | 651 | 80 |
| 6061, O (annealed) | 1,645 | 600 | 250 | 651 | 80 |
| 7075, T6 / T651 | 1,645 | 600 | 250 | 651 | 80 |
| 2024, T3 / T351 | 1,645 | 600 | 250 | 651 | 80 |
| A356 cast aluminum, T6 | 1,645 | 600 | 250 | 651 | 80 |
| 360 brass, Half hard | 1,315 | 400 | 139 | 513 | 72 |
| 932 bearing bronze, As cast | 1,315 | 400 | 139 | 513 | 72 |
| C110 copper, Half hard | — | 400 | 139 | 513 | 72 |
| Ti-6Al-4V, Annealed | 189 | 170 | 39 | 127 | 29 |
| CP titanium, Grade 2, Annealed | 283 | 170 | 39 | 127 | 29 |
| Inconel 718, Solution annealed | 184 | 70 | 15 | 118 | 16 |
| Inconel 718, Aged | 131 | 70 | 15 | 118 | 16 |
| Inconel 625, Annealed | 184 | 70 | 15 | 118 | 16 |
| Hastelloy X, Solution annealed | 184 | 70 | 15 | 118 | 16 |
Starting points from the median of the tool makers' charts; adjust for rigidity, tool and coolant. Turning: medium cut, coated carbide. Drills: Ø1/2" at 3×D. A dash: no maker publishes it. breakingchips.com/cutting-speed-chart/ Version 22 Nov 2026. Free to share under CC BY 4.0: credit BreakingChips (breakingchips.com).