Dowel pin hole sizes
The reamed hole for pressing in a hardened ground dowel pin, the pin's own limits, and the interference between them. No standard table gives a slip-fit hole for the other part, so none is given here; the fits calculator works one out from ISO 286.
Inch hardened ground dowel pins (ASME B18.8.2)
Standard series pins, 0.0002" over nominal. For aluminum or zinc die castings, both hole limits are usually 0.0005" smaller.
| Pin | Press fit hole | Pin Ø | Interference |
|---|---|---|---|
| 1/16" | 0.0620–0.0625" Two published copies agree | Only one published copy | — |
| 5/64" | Only one published copy | Not published | — |
| 3/32" | 0.0932–0.0937" Two published copies agree | Only one published copy | — |
| 1/8" | 0.1245–0.1250" Two published copies agree | Only one published copy | — |
| 5/32" | 0.1557–0.1562" Two published copies agree | Only one published copy | — |
| 3/16" | 0.1870–0.1875" Two published copies agree | Only one published copy | — |
| 1/4" | 0.2495–0.2500" Two published copies agree | 0.2501–0.2503" Two published copies agree | 0.0001–0.0008" |
| 5/16" | 0.3120–0.3125" Two published copies agree | 0.3126–0.3128" Two charts disagree: Unbrako 0.3126–0.3128", Holo-Krome 0.3125–0.3128" | 0.0001–0.0008" |
| 3/8" | 0.3745–0.3750" Two published copies agree | 0.3751–0.3753" Two published copies agree | 0.0001–0.0008" |
| 7/16" | 0.4370–0.4375" Two published copies agree | 0.4376–0.4378" Two published copies agree | 0.0001–0.0008" |
| 1/2" | 0.4995–0.5000" Two published copies agree | 0.5001–0.5003" Two published copies agree | 0.0001–0.0008" |
| 9/16" | Only one published copy | Only one published copy | — |
| 5/8" | 0.6245–0.6250" Two published copies agree | 0.6251–0.6253" Two published copies agree | 0.0001–0.0008" |
| 3/4" | 0.7495–0.7500" Two published copies agree | 0.7501–0.7503" Two published copies agree | 0.0001–0.0008" |
| 7/8" | 0.8745–0.8750" Two published copies agree | Only one published copy | — |
| 1" | 0.9995–1.0000" Two published copies agree | 1.0001–1.0003" Two published copies agree | 0.0001–0.0008" |
Metric dowel pins (ISO 8734)
ISO 8734 sets the pin, not the hole: these holes are Unbrako's recommendation for its own pins.
| Pin | Press fit hole | Pin Ø | Interference |
|---|---|---|---|
| 3 mm | 2.987–3.000 mm One source: Unbrako, the dowel pin maker | 3.003–3.008 mm One source: Unbrako, the dowel pin maker | 0.003–0.021 mm |
| 4 mm | 3.987–4.000 mm One source: Unbrako, the dowel pin maker | 4.004–4.009 mm One source: Unbrako, the dowel pin maker | 0.004–0.022 mm |
| 5 mm | 4.987–5.000 mm One source: Unbrako, the dowel pin maker | 5.004–5.009 mm One source: Unbrako, the dowel pin maker | 0.004–0.022 mm |
| 6 mm | 5.987–6.000 mm One source: Unbrako, the dowel pin maker | 6.004–6.010 mm One source: Unbrako, the dowel pin maker | 0.004–0.023 mm |
| 8 mm | 7.987–8.000 mm One source: Unbrako, the dowel pin maker | 8.006–8.012 mm One source: Unbrako, the dowel pin maker | 0.006–0.025 mm |
| 10 mm | 9.987–10.000 mm One source: Unbrako, the dowel pin maker | 10.006–10.012 mm One source: Unbrako, the dowel pin maker | 0.006–0.025 mm |
| 12 mm | 11.985–12.000 mm One source: Unbrako, the dowel pin maker | 12.007–12.013 mm One source: Unbrako, the dowel pin maker | 0.007–0.028 mm |
| 16 mm | 15.985–16.000 mm One source: Unbrako, the dowel pin maker | 16.007–16.013 mm One source: Unbrako, the dowel pin maker | 0.007–0.028 mm |
| 20 mm | 19.983–20.000 mm One source: Unbrako, the dowel pin maker | 20.008–20.014 mm One source: Unbrako, the dowel pin maker | 0.008–0.031 mm |
| 25 mm | 24.983–25.000 mm One source: Unbrako, the dowel pin maker | 25.008–25.014 mm One source: Unbrako, the dowel pin maker | 0.008–0.031 mm |
Sources3
- Unbrako, Engineering Guide: socket screw products (dimensions, drill and counterbore sizes, dowel pins) (archived Apr 19, 2024)
- Engineers Edge, press fit holes for hardened ground machine dowel pins (ASME B18.8.2) (archived Oct 5, 2024)
- Holo-Krome, product standard HK.USA.DP.SPRL.BO (dowel pin diameters) (archived Nov 12, 2026)