Fractional drill

13/16" drill size

A 13/16" drill is 0.8125" (20.638 mm), the chart tap drill for 7/8-14 UNF; the nearest metric drill is 20.5 mm (0.8071"). It is a cut-tap drill for 7/8-14 UNF (67% thread) and M22 × 1.5 (70% thread).

13/16 drill, Ø.8125 in, with a 118° point .2441 in long.Ø.8125 inlipflutepoint angle 118°point length .2441 in
The point end of a general-purpose twist drill, with the 118° point both makers' catalogs give for general-purpose drilling. Drill drawn about 1.5× its true size. The point is to scale with the body.

Only two makers publish this: ICS Cutting Tools and YG-1

Inch

0.8125"

Metric

20.638 mm

Nearest metric drills: 20.5 mm (0.8071") and 21 mm (0.8268")

Checked against 3 published copies

Other sizes

Threads it taps

Chart tap drill for: 7/8-14 UNF (67%, cut tap)

Suggested: 7/8-14 UNF (67%, cut tap) · M22 × 1.5 (70%, cut tap)

Every thread it taps, 50–85%

Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.

Cut tap

Threads this drill taps with a cutting tap.

Cut tap threads for a 13/16" drill
ThreadThread %
7/8-14 UNFsuggested67%
M22 × 252%
M22 × 1.5suggested70%

Form tap

A form (roll) tap displaces metal, so it takes a bigger hole for the same thread.

Form tap threads for a 13/16" drill
ThreadThread %
7/8-9 UNC83%
M22 × 2.580%
Speeds and feeds for the 13/16" drill

Sources

Sources8