Metric drill

2.2 mm drill size

2.2 mm is 0.0866"; the nearest inch drill is #44 (0.0860"), and the nearest fraction is 3/32" (0.0938"). It is a cut-tap drill for M2.5 × 0.35 (66% thread).

2.2 mm drill, Ø2.200 mm, with a 118° point 0.661 mm long.Ø2.200 mmlipflutepoint angle 118°point length 0.661 mm
The point end of a general-purpose twist drill, with the 118° point both makers' catalogs give for general-purpose drilling. Drill drawn about 14× its true size. The point is to scale with the body.

Only two makers publish this: ICS Cutting Tools and YG-1

Inch

0.0866"

2.2 mm ÷ 25.4, rounded to four places

Nearest inch drill

#44 0.0860"

0.0006" under (0.016 mm)

Checked against 3 published copies

Other sizes

Threads it taps

Suggested: M2.5 × 0.35 (66%, cut tap)

Every thread it taps, 50–85%

Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.

Cut tap

Threads this drill taps with a cutting tap.

Cut tap threads for a 2.2 mm drill
ThreadThread %
#3-56 UNF53%
#4-40 UNC78%
M2.5 × 0.4551%
M2.5 × 0.35suggested66%
Speeds and feeds for the 2.2 mm drill

Sources

Sources7