Metric drill
6 mm drill size
6 mm is 0.2362"; the nearest inch drill is letter B (0.2380"), and the nearest fraction is 15/64" (0.2344").
Only two makers publish this: ICS Cutting Tools and YG-1
Inch
0.2362"
6 mm ÷ 25.4, rounded to four places
Nearest inch drill
Letter B 0.2380"
0.0018" over (0.045 mm)
Checked against 3 published copies
Other sizes
Threads it taps
Suggested: 1/4-32 UNEF (65%, form tap)
Every thread it taps, 50–85%
Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.
Form tap
A form (roll) tap displaces metal, so it takes a bigger hole for the same thread.
| Thread | Thread % |
|---|---|
| 1/4-28 UNF | 57% |
| 1/4-32 UNEFsuggested | 65% |
Sources
Sources7
- Wikipedia — Drill bit sizes: number and letter gauge table (after ASME B94.11M) (archived Oct 24, 2026)
- Engineers Edge — Drill size chart: number, letter, fractional and metric (archived Oct 29, 2026)
- Newman Tools — Decimal equivalent chart: number, letter and fractional drills (archived Sep 23, 2026)
- ASME B1.1 — Unified Inch Screw Threads (UN and UNR thread form)
- ISO 261 / ISO 262 — ISO general purpose metric screw threads: general plan and selected sizes
- OSG — Tap drill size and pitch diameter limit chart (formula, suggested % of full thread) (archived Aug 23, 2025)
- Cutting Tool Engineering — "Threads will roll": form tap hole size = D − 0.0068 × % / TPI (archived Mar 21, 2025)