Metric drill

8.1 mm drill size

8.1 mm is 0.3189"; the nearest inch drill is letter O (0.3160"), and the nearest fraction is 5/16" (0.3125"). It is a cut-tap drill for 3/8-16 UNC (69% thread).

8.1 mm drill, Ø8.100 mm, with a 118° point 2.433 mm long.Ø8.100 mmlipflutepoint angle 118°point length 2.433 mm
The point end of a general-purpose twist drill, with the 118° point both makers' catalogs give for general-purpose drilling. Drill drawn about 4× its true size. The point is to scale with the body.

Only two makers publish this: ICS Cutting Tools and YG-1

Inch

0.3189"

8.1 mm ÷ 25.4, rounded to four places

Nearest inch drill

Letter O 0.3160"

0.0029" under (0.074 mm)

Checked against 3 published copies

Other sizes

Threads it taps

Suggested: 3/8-16 UNC (69%, cut tap)

Every thread it taps, 50–85%

Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.

Cut tap

Threads this drill taps with a cutting tap.

Cut tap threads for a 8.1 mm drill
ThreadThread %
3/8-16 UNCsuggested69%
Speeds and feeds for the 8.1 mm drill

Sources

Sources7