Letter drill

Letter J drill size

A letter J drill is 0.2770" (7.036 mm); the nearest fraction is 9/32" (0.2813"), and the nearest metric drill is 7 mm (0.2756"). It is a cut-tap drill for 5/16-24 UNF (66% thread).

J drill, Ø.2770 in, with a 118° point .0832 in long.Ø.2770 inlipflutepoint angle 118°point length .0832 in
The point end of a general-purpose twist drill, with the 118° point both makers' catalogs give for general-purpose drilling. Drill drawn about 5× its true size. The point is to scale with the body.

Only two makers publish this: ICS Cutting Tools and YG-1

Inch

0.2770"

Between 17/64" (0.2656") and 9/32" (0.2813")

Metric

7.036 mm

Nearest metric drills: 7 mm (0.2756") and 7.1 mm (0.2795")

Checked against 3 published copies

Other sizes

Threads it taps

Suggested: 5/16-24 UNF (66%, cut tap)

Every thread it taps, 50–85%

Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.

Cut tap

Threads this drill taps with a cutting tap.

Cut tap threads for a Letter J drill
ThreadThread %
5/16-24 UNFsuggested66%
M8 × 1.2559%
M8 × 174%
Speeds and feeds for the letter J drill

Sources

Sources8