Letter drill

Letter S drill size

A letter S drill is 0.3480" (8.839 mm); the nearest fraction is 11/32" (0.3438"), and the nearest metric drill is 8.8 mm (0.3465"). It is a cut-tap drill for 3/8-32 UNEF (67% thread).

S drill, Ø.3480 in, with a 118° point .1045 in long.Ø.3480 inlipflutepoint angle 118°point length .1045 in
The point end of a general-purpose twist drill, with the 118° point both makers' catalogs give for general-purpose drilling. Drill drawn about 4× its true size. The point is to scale with the body.

Only two makers publish this: ICS Cutting Tools and YG-1

Inch

0.3480"

Between 11/32" (0.3438") and 23/64" (0.3594")

Metric

8.839 mm

Nearest metric drills: 8.8 mm (0.3465") and 8.9 mm (0.3504")

Checked against 3 published copies

Other sizes

Threads it taps

Suggested: 3/8-32 UNEF (67%, cut tap) · 3/8-16 UNC (64%, form tap)

Every thread it taps, 50–85%

Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.

Cut tap

Threads this drill taps with a cutting tap.

Cut tap threads for a Letter S drill
ThreadThread %
3/8-32 UNEFsuggested67%
M10 × 1.560%
M10 × 1.2571%

Form tap

A form (roll) tap displaces metal, so it takes a bigger hole for the same thread.

Form tap threads for a Letter S drill
ThreadThread %
3/8-16 UNCsuggested64%
Speeds and feeds for the letter S drill

Sources

Sources8