Letter drill

Letter U drill size

A letter U drill is 0.3680" (9.347 mm), the chart tap drill for 7/16-14 UNC; the nearest fraction is 3/8" (0.3750"), and the nearest metric drill is 9.3 mm (0.3661"). It is a cut-tap drill for M10 × 0.75 (67% thread).

U drill, Ø.3680 in, with a 118° point .1106 in long.Ø.3680 inlipflutepoint angle 118°point length .1106 in
The point end of a general-purpose twist drill, with the 118° point both makers' catalogs give for general-purpose drilling. Drill drawn about 3× its true size. The point is to scale with the body.

Only two makers publish this: ICS Cutting Tools and YG-1

Inch

0.3680"

Between 23/64" (0.3594") and 3/8" (0.3750")

Metric

9.347 mm

Nearest metric drills: 9.3 mm (0.3661") and 9.4 mm (0.3701")

Checked against 3 published copies

Other sizes

Threads it taps

Chart tap drill for: 7/16-14 UNC (75%, cut tap)

Suggested: M10 × 0.75 (67%, cut tap)

Every thread it taps, 50–85%

Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.

Cut tap

Threads this drill taps with a cutting tap.

Cut tap threads for a Letter U drill
ThreadThread %
7/16-14 UNC75%
M10 × 150%
M10 × 0.75suggested67%

Form tap

A form (roll) tap displaces metal, so it takes a bigger hole for the same thread.

Form tap threads for a Letter U drill
ThreadThread %
M10 × 1.564%
M10 × 1.2577%
Speeds and feeds for the letter U drill

Sources

Sources8