Number drill
#13 drill size
A #13 drill is 0.1850" (4.699 mm); the nearest fraction is 3/16" (0.1875"), and the nearest metric drill is 4.7 mm (0.1850"). It is a cut-tap drill for #12-28 UNF (67% thread).
Only two makers publish this: ICS Cutting Tools and YG-1
Inch
0.1850"
Between 11/64" (0.1719") and 3/16" (0.1875")
Metric
4.699 mm
Nearest metric drills: 4.6 mm (0.1811") and 4.7 mm (0.1850")
Checked against 3 published copies
Other sizes
Threads it taps
Suggested: #12-28 UNF (67%, cut tap)
Every thread it taps, 50–85%
Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.
Cut tap
Threads this drill taps with a cutting tap.
| Thread | Thread % |
|---|---|
| #12-24 UNC | 57% |
| #12-28 UNFsuggested | 67% |
| #12-32 UNEF | 76% |
Form tap
A form (roll) tap displaces metal, so it takes a bigger hole for the same thread.
| Thread | Thread % |
|---|---|
| M5 × 0.8 | 55% |
Sources
Sources8
- ASME B94.11M — Twist drills (fractional, number, letter and metric sizes)
- Wikipedia — Drill bit sizes: number and letter gauge table (after ASME B94.11M) (archived Oct 24, 2026)
- Engineers Edge — Drill size chart: number, letter, fractional and metric (archived Oct 29, 2026)
- Newman Tools — Decimal equivalent chart: number, letter and fractional drills (archived Sep 23, 2026)
- ASME B1.1 — Unified Inch Screw Threads (UN and UNR thread form)
- ISO 261 / ISO 262 — ISO general purpose metric screw threads: general plan and selected sizes
- OSG — Tap drill size and pitch diameter limit chart (formula, suggested % of full thread) (archived Aug 23, 2025)
- Cutting Tool Engineering — "Threads will roll": form tap hole size = D − 0.0068 × % / TPI (archived Mar 21, 2025)