Number drill
#53 drill size
A #53 drill is 0.0595" (1.511 mm), the chart tap drill for #1-64 UNC and #1-72 UNF; the nearest fraction is 1/16" (0.0625"), and the nearest metric drill is 1.5 mm (0.0591"). It is a cut-tap drill for #1-64 UNC (67% thread) and #1-72 UNF (75% thread).
Only two makers publish this: ICS Cutting Tools and YG-1
Inch
0.0595"
Between 3/64" (0.0469") and 1/16" (0.0625")
Metric
1.511 mm
Nearest metric drills: 1.5 mm (0.0591") and 1.6 mm (0.0630")
Checked against 3 published copies
Other sizes
Threads it taps
Chart tap drill for: #1-64 UNC (67%, cut tap) · #1-72 UNF (75%, cut tap)
Suggested: #1-64 UNC (67%, cut tap) · #1-72 UNF (75%, cut tap) · M1.6 × 0.2 (65%, form tap)
Every thread it taps, 50–85%
Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.
Cut tap
Threads this drill taps with a cutting tap.
Form tap
A form (roll) tap displaces metal, so it takes a bigger hole for the same thread.
| Thread | Thread % |
|---|---|
| M1.6 × 0.2suggested | 65% |
Sources
Sources8
- ASME B94.11M — Twist drills (fractional, number, letter and metric sizes)
- Wikipedia — Drill bit sizes: number and letter gauge table (after ASME B94.11M) (archived Oct 24, 2026)
- Engineers Edge — Drill size chart: number, letter, fractional and metric (archived Oct 29, 2026)
- Newman Tools — Decimal equivalent chart: number, letter and fractional drills (archived Sep 23, 2026)
- ASME B1.1 — Unified Inch Screw Threads (UN and UNR thread form)
- ISO 261 / ISO 262 — ISO general purpose metric screw threads: general plan and selected sizes
- OSG — Tap drill size and pitch diameter limit chart (formula, suggested % of full thread) (archived Aug 23, 2025)
- Cutting Tool Engineering — "Threads will roll": form tap hole size = D − 0.0068 × % / TPI (archived Mar 21, 2025)