Number drill
#69 drill size
A #69 drill is 0.0292" (0.742 mm); the nearest fraction is 1/32" (0.0313"), and the nearest metric drill is 0.7 mm (0.0276"). It is a cut-tap drill for M1 × 0.25 (80% thread).
Only two makers publish this: ICS Cutting Tools and YG-1
Inch
0.0292"
Between 1/64" (0.0156") and 1/32" (0.0313")
Metric
0.742 mm
Nearest metric drills: 0.7 mm (0.0276") and 0.8 mm (0.0315")
Checked against 3 published copies
Other sizes
Threads it taps
Suggested: M1 × 0.25 (80%, cut tap)
Every thread it taps, 50–85%
Every standard UN and ISO metric thread this drill gives 50–85% of full thread. Suggested rows are in OSG's 65–70% band for general work.
Cut tap
Threads this drill taps with a cutting tap.
| Thread | Thread % |
|---|---|
| M1 × 0.25suggested | 80% |
Sources
Sources8
- ASME B94.11M — Twist drills (fractional, number, letter and metric sizes)
- Wikipedia — Drill bit sizes: number and letter gauge table (after ASME B94.11M) (archived Oct 24, 2026)
- Engineers Edge — Drill size chart: number, letter, fractional and metric (archived Oct 29, 2026)
- Newman Tools — Decimal equivalent chart: number, letter and fractional drills (archived Sep 23, 2026)
- ASME B1.1 — Unified Inch Screw Threads (UN and UNR thread form)
- ISO 261 / ISO 262 — ISO general purpose metric screw threads: general plan and selected sizes
- OSG — Tap drill size and pitch diameter limit chart (formula, suggested % of full thread) (archived Aug 23, 2025)
- Cutting Tool Engineering — "Threads will roll": form tap hole size = D − 0.0068 × % / TPI (archived Mar 21, 2025)