Number drill
#73 drill size
A #73 drill is 0.0240" (0.610 mm); the nearest fraction is 1/32" (0.0313"), and the nearest metric drill is 0.6 mm (0.0236").
Only two makers publish this: ICS Cutting Tools and YG-1
Inch
0.0240"
Between 1/64" (0.0156") and 1/32" (0.0313")
Metric
0.610 mm
Nearest metric drills: 0.6 mm (0.0236") and 0.7 mm (0.0276")
Checked against 3 published copies
Other sizes
Threads it taps
This drill doesn't give 50–85% of thread for any standard UN or ISO metric thread.
Sources
Sources4
- ASME B94.11M — Twist drills (fractional, number, letter and metric sizes)
- Wikipedia — Drill bit sizes: number and letter gauge table (after ASME B94.11M) (archived Oct 24, 2026)
- Engineers Edge — Drill size chart: number, letter, fractional and metric (archived Oct 29, 2026)
- Newman Tools — Decimal equivalent chart: number, letter and fractional drills (archived Sep 23, 2026)