88-piece inch gauge block set

An 88-piece inch gauge block set holds 9 blocks .1001" to .1009" by .0001", 49 blocks .101" to .149" by .001", 19 blocks .050" to .950" by .050", 4 blocks 1.000" to 4.000" by 1", 3 blocks .100025", .10005" and .100075" and 4 blocks 1/16", 5/64", 3/32" and 7/64". This is Starrett-Webber’s set. Example: 1.0625" = .0625 + 1.0000, two blocks.

Build a stack from this set →

A 1.0625" stack of gauge blocks, wrung together: .0625 + 1.0000.1.0625"gauge block1.0000".0625"
The 1.0625" stack from the 88-piece inch set. To scale.

What’s in the box

88-piece inch gauge block set contents
BlocksCount
.1001" to .1009" by .0001"9
.101" to .149" by .001"49
.050" to .950" by .050"19
1.000" to 4.000" by 1"4
.100025", .10005" and .100075"3
1/16", 5/64", 3/32" and 7/64"4

Total: 88 blocks.

Mitutoyo has no 88-piece inch set; its 92-piece set holds the same seven extra blocks.

Every block, thinnest first

.0500, .0625, .078125, .09375, .1000, .100025, .10005, .100075, .1001, .1002, .1003, .1004, .1005, .1006, .1007, .1008, .1009, .1010, .1020, .1030, .1040, .1050, .1060, .1070, .1080, .1090, .109375, .1100, .1110, .1120, .1130, .1140, .1150, .1160, .1170, .1180, .1190, .1200, .1210, .1220, .1230, .1240, .1250, .1260, .1270, .1280, .1290, .1300, .1310, .1320, .1330, .1340, .1350, .1360, .1370, .1380, .1390, .1400, .1410, .1420, .1430, .1440, .1450, .1460, .1470, .1480, .1490, .1500, .2000, .2500, .3000, .3500, .4000, .4500, .5000, .5500, .6000, .6500, .7000, .7500, .8000, .8500, .9000, .9500, 1.0000, 2.0000, 3.0000, 4.0000

One source: Starrett-Webber, the maker of this set

Worked stacks

Example stacks from the 88-piece inch set
HeightBlocksCount
1.0625".0625 + 1.00002
.200025".100025 + .10002
2.4567".1007 + .1060 + .2500 + 2.00004

Found by the stack calculator: the fewest blocks, finest digit first. Each row opens it with that height.

On the bench

Show

Wring the blocks, don’t just stack them: slide each one onto the next with light pressure until it grabs, so there’s no air gap. If you use the stack a lot, put a wear block on each end (.050" or .100" pairs are sold for it) and take them out of the height first. Handle blocks by the edges, and give a stack a few minutes to come back to room temperature after it’s been in your hand: warm steel is longer.

Sources1