ASTM E140 · Non-austenitic steel
20 HRC to HV and HB (ASTM E140)
By ASTM E140 Table 1, 20 HRC equals 238 HV (Vickers) and 226 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.
- Brinell
- 226 HB
10 mm carbide ball, 3000 kgf (HBW)
- Vickers
- 238 HV
- Rockwell B
- 99.7 HRB
Read from Table 2 by Vickers, between its rows; the two scales meet here
Checked against 3 published copies
Nearby values
Sources
Sources8
ASTM E140, Standard Hardness Conversion Tables for Metals, Tables 1 and 2 (non-austenitic steels). Every value on this page was checked against these published copies:
- Phase II — Rockwell C hardness conversion chart (ASTM E140 Table 1) (archived May 13, 2026)
- LabTesting — Rockwell C hardness conversion, non-austenitic steels (archived Jul 13, 2026)
- NSM — Hardness conversion calculator (ASTM E140 Tables 1 and 2) (archived Nov 16, 2026)
- Misumi — Conversion table of hardness, SAE J417 (from ASTM E140 Table 1) (archived Nov 15, 2026)
- Honesdom (hardnessgauge.com) — Hardness conversion chart, Rockwell C (archived May 15, 2026)
- Phase II — Rockwell B hardness conversion chart (ASTM E140 Table 2) (archived May 13, 2026)
- LabTesting — Rockwell B hardness conversion, non-austenitic steels (archived Jun 26, 2024)
- Honesdom (hardnessgauge.com) — Hardness conversion chart, Rockwell B (archived May 15, 2026)