Printable hardness conversion chart
Back to the full chart
One page on Letter or A4. To save a PDF, pick "Save as PDF" in the print dialog.
| HRC | HV | HB |
|---|---|---|
| 68 HRC | 940 | — |
| 67 HRC | 900 | — |
| 66 HRC | 865 | — |
| 65 HRC | 832 | (739) |
| 64 HRC | 800 | (722) |
| 63 HRC | 772 | (705) |
| 62 HRC | 746 | (688) |
| 61 HRC | 720 | (670) |
| 60 HRC | 697 | (654) |
| 59 HRC | 674 | 634 |
| 58 HRC | 653 | 615 |
| 57 HRC | 633 | 595 |
| 56 HRC | 613 | 577 |
| 55 HRC | 595 | 560 |
| 54 HRC | 577 | 543 |
| 53 HRC | 560 | 525 |
| 52 HRC | 544 | 512 |
| 51 HRC | 528 | 496 |
| 50 HRC | 513 | 481 |
| 49 HRC | 498 | 469 |
| 48 HRC | 484 | 455 |
| 47 HRC | 471 | 443 |
| 46 HRC | 458 | 432 |
| 45 HRC | 446 | 421 |
| 44 HRC | 434 | 409 |
| 43 HRC | 423 | 400 |
| 42 HRC | 412 | 390 |
| 41 HRC | 402 | 381 |
| 40 HRC | 392 | 371 |
| 39 HRC | 382 | 362 |
| 38 HRC | 372 | 353 |
| 37 HRC | 363 | 344 |
| 36 HRC | 354 | 336 |
| 35 HRC | 345 | 327 |
| 34 HRC | 336 | 319 |
| 33 HRC | 327 | 311 |
| 32 HRC | 318 | 301 |
| 31 HRC | 310 | 294 |
| 30 HRC | 302 | 286 |
| 29 HRC | 294 | 279 |
| 28 HRC | 286 | 271 |
| 27 HRC | 279 | 264 |
| 26 HRC | 272 | 258 |
| 25 HRC | 266 | 253 |
| 24 HRC | 260 | 247 |
| 23 HRC | 254 | 243 |
| 22 HRC | 248 | 237 |
| 21 HRC | 243 | 231 |
| 20 HRC | 238 | 226 |
| HRB | HV | HB |
|---|---|---|
| 100 HRB | 240 | 240 |
| 99 HRB | 234 | 234 |
| 98 HRB | 228 | 228 |
| 97 HRB | 222 | 222 |
| 96 HRB | 216 | 216 |
| 95 HRB | 210 | 210 |
| 94 HRB | 205 | 205 |
| 93 HRB | 200 | 200 |
| 92 HRB | 195 | 195 |
| 91 HRB | 190 | 190 |
| 90 HRB | 185 | 185 |
| 89 HRB | 180 | 180 |
| 88 HRB | 176 | 176 |
| 87 HRB | 172 | 172 |
| 86 HRB | 169 | 169 |
| 85 HRB | 165 | 165 |
| 84 HRB | 162 | 162 |
| 83 HRB | 159 | 159 |
| 82 HRB | 156 | 156 |
| 81 HRB | 153 | 153 |
| 80 HRB | 150 | 150 |
| 79 HRB | 147 | 147 |
| 78 HRB | 144 | 144 |
| 77 HRB | 141 | 141 |
| 76 HRB | 139 | 139 |
| 75 HRB | 137 | 137 |
| 74 HRB | 135 | 135 |
| 73 HRB | 132 | 132 |
| 72 HRB | 130 | 130 |
| 71 HRB | 127 | 127 |
| 70 HRB | 125 | 125 |
| 69 HRB | 123 | 123 |
| 68 HRB | 121 | 121 |
| 67 HRB | 119 | 119 |
| 66 HRB | 117 | 117 |
| 65 HRB | 116 | 116 |
| 64 HRB | 114 | 114 |
| 63 HRB | 112 | 112 |
| 62 HRB | 110 | 110 |
| 61 HRB | 108 | 108 |
| 60 HRB | 107 | 107 |
ASTM E140, non-austenitic steel; approximate by the standard's own words. Brinell: 10 mm carbide ball (HRC), steel ball (HRB), 3000 kgf. breakingchips.com/calculators/hardness/ Version 22 Nov 2026. Free to share under CC BY 4.0: credit BreakingChips (breakingchips.com).