Heli-Coil insert · #12-24 UNC
#12-24 Helicoil drill size
The Heli-Coil drill for #12-24 is #1 (0.2280", 5.79 mm) in aluminum and steel. Countersink 120°, then tap with the #12-24 STI tap, not the standard #12-24 tap: the insert's wire needs a hole 0.0541" bigger on every diameter.
Aluminum
#1
0.2280" · 5.79 mm
Steel, magnesium, plastic
#1
0.2280" · 5.79 mm
One source: Heli-Coil, the insert’s maker (HC-2000)
#12-24 STI thread (tapped hole, minimum)
- Major Ø
- 0.270" (6.86 mm)
- Pitch Ø
- 0.243" (6.17 mm)
- Minor Ø
- 0.225" (5.72 mm)
- Threads per inch
- 24
How these are worked
Each is the #12-24 UNC basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.
Two published copies agree
Minimum tapping depth
Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.
| Insert | Insert length | Tap at least |
|---|---|---|
| 1 × D | 0.216" | 0.258" |
| 1.5 × D | 0.324" | 0.366" |
| 2 × D | 0.432" | 0.474" |
| 2.5 × D | 0.540" | 0.582" |
| 3 × D | 0.648" | 0.690" |
One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)
Sources
Sources3
- Stanley Engineered Fastening — Heli-Coil inserts, HC-2000 rev 11: Tables V–VIII, drilled and tapped hole dimensions (archived Nov 25, 2024)
- Amesweb — Helicoil tap sizes (STI), after ASME B18.29.1 (archived Jul 11, 2026)
- ASME B18.29.1 — Helical coil screw thread inserts, free running and screw locking (inch series)