Heli-Coil insert · #3-56 UNF
#3-56 Helicoil drill size
The Heli-Coil drill for #3-56 is #37 (0.1040", 2.64 mm) in aluminum and #36 (0.1065", 2.71 mm) in steel. Countersink 120°, then tap with the #3-56 STI tap, not the standard #3-56 tap: the insert's wire needs a hole 0.0232" bigger on every diameter.
Aluminum
#37
0.1040" · 2.64 mm
Steel, magnesium, plastic
#36
0.1065" · 2.71 mm
One source: Heli-Coil, the insert’s maker (HC-2000)
#3-56 STI thread (tapped hole, minimum)
- Major Ø
- 0.122" (3.10 mm)
- Pitch Ø
- 0.111" (2.81 mm)
- Minor Ø
- 0.103" (2.61 mm)
- Threads per inch
- 56
How these are worked
Each is the #3-56 UNF basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.
Two published copies agree
Minimum tapping depth
Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.
| Insert | Insert length | Tap at least |
|---|---|---|
| 1 × D | 0.099" | 0.117" |
| 1.5 × D | 0.149" | 0.166" |
| 2 × D | 0.198" | 0.216" |
| 2.5 × D | 0.248" | 0.265" |
| 3 × D | 0.297" | 0.315" |
One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)
Sources
Sources3
- Stanley Engineered Fastening — Heli-Coil inserts, HC-2000 rev 11: Tables V–VIII, drilled and tapped hole dimensions (archived Nov 25, 2024)
- Amesweb — Helicoil tap sizes (STI), after ASME B18.29.1 (archived Jul 11, 2026)
- ASME B18.29.1 — Helical coil screw thread inserts, free running and screw locking (inch series)