Heli-Coil insert · 5/8-11 UNC

5/8-11 Helicoil drill size

The Heli-Coil drill for 5/8-11 is 21/32" (0.6563", 16.67 mm) in aluminum and steel. Countersink 120°, then tap with the 5/8-11 STI tap, not the standard 5/8-11 tap: the insert's wire needs a hole 0.1181" bigger on every diameter.

A 5/8-11 Heli-Coil in its STI-tapped hole, in section: the insert's coils in the STI thread, the tang across the bore at the bottom.STI tap 5/8-11inserttangSTI drill 21/32
A 5/8-11 Heli-Coil in its STI-tapped hole. Diameters and pitch to scale; the hole’s depth is not.

Aluminum

21/32

0.6563" · 16.67 mm

Steel, magnesium, plastic

21/32

0.6563" · 16.67 mm

One source: Heli-Coil, the insert’s maker (HC-2000)

5/8-11 STI thread (tapped hole, minimum)

Major Ø
0.743" (18.87 mm)
Pitch Ø
0.684" (17.37 mm)
Minor Ø
0.645" (16.37 mm)
Threads per inch
11
How these are worked

Each is the 5/8-11 UNC basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.

Two published copies agree

Minimum tapping depth

Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.

5/8-11 UNC STI minimum tapping depth by insert length
InsertInsert lengthTap at least
1 × D0.625"0.716"
1.5 × D0.938"1.028"
2 × D1.250"1.341"
2.5 × D1.563"1.653"
3 × D1.875"1.966"

One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)

Sources

Sources3