Heli-Coil insert · M10 × 1.25
M10 × 1.25 Helicoil drill size
The Heli-Coil drill for M10 × 1.25 is 10.25 mm (0.4035") in aluminum and steel. Countersink 120°, then tap with the M10 × 1.25 STI tap, not the standard M10 × 1.25 tap: the insert's wire needs a hole 1.624 mm bigger on every diameter.
Aluminum
10.25 mm
0.4035"
Steel, magnesium, plastic
10.25 mm
0.4035"
One source: Heli-Coil, the insert’s maker (HC-2000)
M10 × 1.25 STI thread (tapped hole, minimum)
- Major Ø
- 11.62 mm (0.458")
- Pitch Ø
- 10.81 mm (0.426")
- Minor Ø
- 10.27 mm (0.404")
- Pitch
- 1.25 mm
How these are worked
Each is the M10 × 1.25 basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.
One source: Heli-Coil, the insert’s maker (HC-2000 Table VIII)
Minimum tapping depth
Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.
| Insert | Insert length | Tap at least |
|---|---|---|
| 1 × D | 10.00 mm | 11.25 mm |
| 1.5 × D | 15.00 mm | 16.25 mm |
| 2 × D | 20.00 mm | 21.25 mm |
| 2.5 × D | 25.00 mm | 26.25 mm |
| 3 × D | 30.00 mm | 31.25 mm |
One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)