Heli-Coil insert · M12 × 1.5
M12 × 1.5 Helicoil drill size
The Heli-Coil drill for M12 × 1.5 is 12.25 mm (0.4823") in aluminum and 12.5 mm (0.4921") in steel. Countersink 120°, then tap with the M12 × 1.5 STI tap, not the standard M12 × 1.5 tap: the insert's wire needs a hole 1.949 mm bigger on every diameter.
Aluminum
12.25 mm
0.4823"
Steel, magnesium, plastic
12.5 mm
0.4921"
One source: Heli-Coil, the insert’s maker (HC-2000)
M12 × 1.5 STI thread (tapped hole, minimum)
- Major Ø
- 13.95 mm (0.549")
- Pitch Ø
- 12.97 mm (0.511")
- Minor Ø
- 12.32 mm (0.485")
- Pitch
- 1.5 mm
How these are worked
Each is the M12 × 1.5 basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.
One source: Heli-Coil, the insert’s maker (HC-2000 Table VIII)
Minimum tapping depth
Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.
| Insert | Insert length | Tap at least |
|---|---|---|
| 1 × D | 12.00 mm | 13.50 mm |
| 1.5 × D | 18.00 mm | 19.50 mm |
| 2 × D | 24.00 mm | 25.50 mm |
| 2.5 × D | 30.00 mm | 31.50 mm |
| 3 × D | 36.00 mm | 37.50 mm |
One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)