Heli-Coil insert · M12 × 1.75

M12 × 1.75 Helicoil drill size

The Heli-Coil drill for M12 × 1.75 is 12.5 mm (0.4921") in aluminum and steel. Countersink 120°, then tap with the M12 × 1.75 STI tap, not the standard M12 × 1.75 tap: the insert's wire needs a hole 2.273 mm bigger on every diameter.

A M12 × 1.75 Heli-Coil in its STI-tapped hole, in section: the insert's coils in the STI thread, the tang across the bore at the bottom.STI tap M12 × 1.75inserttangSTI drill 12.5 mm
A M12 × 1.75 Heli-Coil in its STI-tapped hole. Diameters and pitch to scale; the hole’s depth is not.

Aluminum

12.5 mm

0.4921"

Steel, magnesium, plastic

12.5 mm

0.4921"

One source: Heli-Coil, the insert’s maker (HC-2000)

M12 × 1.75 STI thread (tapped hole, minimum)

Major Ø
14.27 mm (0.562")
Pitch Ø
13.14 mm (0.517")
Minor Ø
12.38 mm (0.487")
Pitch
1.75 mm
How these are worked

Each is the M12 × 1.75 basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.

One source: Heli-Coil, the insert’s maker (HC-2000 Table VIII)

Minimum tapping depth

Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.

M12 × 1.75 STI minimum tapping depth by insert length
InsertInsert lengthTap at least
1 × D12.00 mm13.75 mm
1.5 × D18.00 mm19.75 mm
2 × D24.00 mm25.75 mm
2.5 × D30.00 mm31.75 mm
3 × D36.00 mm37.75 mm

One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)

Sources

Sources1