Heli-Coil insert · M22 × 1.5

M22 × 1.5 Helicoil drill size

The Heli-Coil drill for M22 × 1.5 is 22.25 mm (0.8760") in aluminum and 22.5 mm (0.8858") in steel. Countersink 120°, then tap with the M22 × 1.5 STI tap, not the standard M22 × 1.5 tap: the insert's wire needs a hole 1.949 mm bigger on every diameter.

A M22 × 1.5 Heli-Coil in its STI-tapped hole, in section: the insert's coils in the STI thread, the tang across the bore at the bottom.STI tap M22 × 1.5inserttangSTI drill 22.25 mm / 22.5 mm
A M22 × 1.5 Heli-Coil in its STI-tapped hole. Diameters and pitch to scale; the hole’s depth is not.

Aluminum

22.25 mm

0.8760"

Steel, magnesium, plastic

22.5 mm

0.8858"

One source: Heli-Coil, the insert’s maker (HC-2000)

M22 × 1.5 STI thread (tapped hole, minimum)

Major Ø
23.95 mm (0.943")
Pitch Ø
22.97 mm (0.904")
Minor Ø
22.32 mm (0.879")
Pitch
1.5 mm
How these are worked

Each is the M22 × 1.5 basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.

One source: Heli-Coil, the insert’s maker (HC-2000 Table VIII)

Minimum tapping depth

Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.

M22 × 1.5 STI minimum tapping depth by insert length
InsertInsert lengthTap at least
1 × D22.00 mm23.50 mm
1.5 × D33.00 mm34.50 mm
2 × D44.00 mm45.50 mm
2.5 × D55.00 mm56.50 mm
3 × D66.00 mm67.50 mm

One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)

Sources

Sources1