Heli-Coil insert · M8 × 1.25

M8 × 1.25 Helicoil drill size

The Heli-Coil drill for M8 × 1.25 is 8.3 mm (0.3268") in aluminum and 8.4 mm (0.3307") in steel. Countersink 120°, then tap with the M8 × 1.25 STI tap, not the standard M8 × 1.25 tap: the insert's wire needs a hole 1.624 mm bigger on every diameter.

A M8 × 1.25 Heli-Coil in its STI-tapped hole, in section: the insert's coils in the STI thread, the tang across the bore at the bottom.STI tap M8 × 1.25inserttangSTI drill 8.3 mm / 8.4 mm
A M8 × 1.25 Heli-Coil in its STI-tapped hole. Diameters and pitch to scale; the hole’s depth is not.

Aluminum

8.3 mm

0.3268"

Steel, magnesium, plastic

8.4 mm

0.3307"

One source: Heli-Coil, the insert’s maker (HC-2000)

M8 × 1.25 STI thread (tapped hole, minimum)

Major Ø
9.62 mm (0.379")
Pitch Ø
8.81 mm (0.347")
Minor Ø
8.27 mm (0.326")
Pitch
1.25 mm
How these are worked

Each is the M8 × 1.25 basic size + 1.299 × pitch. The class of fit (2B, 3B, 4H5H) sets the limits above these.

One source: Heli-Coil, the insert’s maker (HC-2000 Table VIII)

Minimum tapping depth

Full thread, for a countersunk hole: the insert length plus one pitch. Drill deeper for the tap's chamfer.

M8 × 1.25 STI minimum tapping depth by insert length
InsertInsert lengthTap at least
1 × D8.00 mm9.25 mm
1.5 × D12.00 mm13.25 mm
2 × D16.00 mm17.25 mm
2.5 × D20.00 mm21.25 mm
3 × D24.00 mm25.25 mm

One source: Heli-Coil, the insert’s maker (HC-2000 Tables VII–VIII, “C”)

Sources

Sources1