Learn · 8 min

Single-point threading step by step

Single-point threading starts with the setup: turn the blank to the major diameter, chamfer the end, and set a 60° tool on centre, square to the work.

Single-point threading a 1/2-13, in section: the 60° tool in a groove, fed along the compound swung 29.5° off the radial line. Pitch .0769", thread depth .0472", which is .0542" on the compound.tool bitcompound 29.5°infeed .0542"workthread depth .0472"pitch .0769"
A 1/2-13 in section, the tool fed along the compound. Enlarged; the thread form to scale.

Set up

Turn the blank to the thread’s major diameter, or a few thousandths under, and chamfer the end to the thread’s depth so the first thread doesn’t burr. Cut a groove (undercut) at the end of the thread if it runs to a shoulder: it gives the tool somewhere to stop.

Grind or pick a 60° tool and set it on centre height, square to the work with a fishtail (centre) gauge. Set the gearbox to the thread’s TPI or pitch and the lathe to a slow speed: with a manual lathe you need time to open the half nut at the end of the thread.

The compound at 29.5°

Swing the compound about 29 to 29.5° off the cross slide’s line, so feeding it moves the tool in and toward the headstock for a right-hand thread. South Bend says 29.5°, the classic texts 29°, Kennametal 28 to 29.5°.

Why not 30°, or straight in? Fed straight in, both sides of the tool cut at once and the chip jams in the V. Fed along the compound, the leading edge does the cutting. Half a degree less than the 30° flank lets the trailing edge shave the other flank lightly instead of rubbing it.

The compound moves along its own line, so to go one thousandth deeper it moves a little more: depth ÷ cos 29.5°, about 1.15 times. A 1/2-13 thread is .0472" deep, which is .0542" on the compound dial.

Passes

Zero the cross slide and the compound with the tool just touching. Take a scratch pass a thousandth or two deep and check the pitch with a thread gauge or a rule: it is the cheapest moment to catch a wrong gear.

Then cut in passes that get smaller as you go deeper, because a V tool has more edge in the cut the deeper it is. Tool makers print the number of passes for each pitch: for 13 TPI about nine, the first about .009" deep. Back the cross slide out at the end of every pass, return, set it back to zero and feed only the compound.

Finish with a spring pass at the last setting: the tool takes a whisker off where the work sprang away from the cut.

The half nut and the dial

At the end of each pass open the half nut, wind the carriage back, and close it again on the line the thread dial chart gives. On an 8 TPI leadscrew with the usual 16-tooth dial, 13 TPI closes on lines 1 and 3. A metric thread on an inch lathe never comes back into step: leave the half nut closed and reverse the spindle instead.

Check the fit

Near full depth, measure. Three wires of the best size, laid in the thread, let a micrometer read the pitch diameter: over .0444" wires a basic 1/2-13 measures .5167". Or try the nut. Take the last passes a thousandth at a time and measure between them.

On a CNC lathe G76 does all of this in one block: the depth, the first cut, the shrinking passes and the infeed along the flank.

Try it on a calculator

  • Single-point threading calculator — Thread depth, compound setting, passes and infeed, the thread dial for your lathe, a G76 line for Fanuc or Haas, and the wire check.
  • Thread dial calculator — Which line to close the half nut on for any TPI or metric pitch, worked from your leadscrew, dial gear and dial lines.
Check yourself: 5 questions

Check yourself

  1. 1. How deep is a 1/2-13 external thread?

  2. 2. With the compound at 29.5°, what does its dial read at full depth for that thread?

  3. 3. About how many passes do tool makers give a 13 TPI thread?

  4. 4. Why feed along the compound instead of straight in?

  5. 5. Over the best-size wires, what does a basic 1/2-13 measure?

0 of 5 answered