4140 steel vs 4340 steel

4340 steel adds nickel (1.65–2.00 %); 4140 steel’s specification doesn’t call for it.

4140 steel and 4340 steel starting speeds by condition. 4140 steel, ISO group P: annealed, 542 SFM carbide turning, 328 SFM end mill; quenched & tempered (pre-hard, ~28–32 HRC), 394 SFM carbide turning, 238 SFM end mill; hardened 50 HRC, none published. 4340 steel, ISO group P: annealed, 542 SFM carbide turning, 328 SFM end mill; quenched & tempered, 394 SFM carbide turning, 238 SFM end mill; hardened 50 HRC, none published.carbide turningend millP4140 steel, Annealed4340 steel, Annealed542 SFM328 SFM4140 steel, Quenched & tempered4340 steel, Quenched & tempered394 SFM238 SFM
Starting speeds in SFM, the median of the makers that publish them. No published speed for 4140 steel, hardened 50 HRC and 4340 steel, hardened 50 HRC. Bars to one scale on every material page.

Composition, side by side

Weight %. A dash means the standard sets no limit for that element.

  • 4140:

    Two published copies agree

    unless marked
  • 4340:

    Checked against 3 published copies

    unless marked
4140 steel and 4340 steel composition, weight percent
Element41404340
C0.38–0.430.37–0.43 or 0.38–0.43

Published copies disagree: AZoM and Alro 0.37–0.43; Engineering ToolBox 0.38–0.43

Mn0.75–1.000.60–0.80
Si0.15–0.30 or 0.15–0.35

Published copies disagree: AZoM 0.15–0.30; Chicago Tube 0.15–0.35

0.15–0.30
Cr0.80–1.100.70–0.90
Mo0.15–0.250.20–0.30
P0.035 max0.035 max
S0.04 max0.04 max
Ni—1.65–2.00

Starting cutting speeds, SFM

Same group, same starting speeds: makers give starting speeds by ISO group, not by alloy.

The calculators' starting points with no tool or setup picked. Each material page has the feeds and the makers behind them.

Starting cutting speeds in surface feet per minute
Material, conditionTurning, carbideEnd millHSS drill
4140, Annealedand 4340, Annealed54232874
4140, Quenched & tempered (pre-hard, ~28–32 HRC)and 4340, Quenched & tempered39423839
4140, Hardened 50 HRCand 4340, Hardened 50 HRC418——

Every property, sourced

4140 steel: strength, hardness and machinability

4140 steel composition

Weight %, from AISI/SAE 4140. Each limit is checked against its published copies, not averaged.

4140 steel chemical composition, weight percent
ElementLimit, %
C0.38–0.43

Two published copies agree

Mn0.75–1.00

Two published copies agree

Si0.15–0.30 or 0.15–0.35

Published copies disagree: AZoM 0.15–0.30; Chicago Tube 0.15–0.35

Cr0.80–1.10

Two published copies agree

Mo0.15–0.25

Two published copies agree

P0.035 max

Two published copies agree

S0.04 max

Two published copies agree

4140 steel mechanical properties

By condition. Typical values vary by mill and bar size; specified minimums are what the standard guarantees.

Hot rolled, annealed, typical

Tensile strength, typical
Not enough published data yet
Yield strength (0.2 %), typical
Not enough published data yet
Elongation in 2 in., typical
Not enough published data yet
Hardness, HB
192 HB

Only two makers publish this: AZoM and Speedy Metals

Cold finished, annealed, typical

Tensile strength, typical
110 ksi · 755 MPa105–114 ksi

Only two makers publish this: Chicago Tube and Specialty Steel

Yield strength (0.2 %), typical
93 ksi · 639 MPa85–101 ksi

Only two makers publish this: Chicago Tube and Specialty Steel

Elongation in 2 in., typical
Not enough published data yet
Hardness, HB
211 HB

Only two makers publish this: Chicago Tube and Specialty Steel

Machinability ratings

Each as its publisher prints it, with the baseline it is measured against. Ratings on different baselines are not comparable, so none are averaged.

  • 65 % (AISI 1212 = 100, annealed): AZoM
  • 63 % (AISI B1112 = 100, hot rolled, annealed): Speedy Metals
4340 steel: strength, hardness and machinability

4340 steel composition

Weight %, from AISI/SAE 4340. Each limit is checked against its published copies, not averaged.

4340 steel chemical composition, weight percent
ElementLimit, %
C0.37–0.43 or 0.38–0.43

Published copies disagree: AZoM and Alro 0.37–0.43; Engineering ToolBox 0.38–0.43

Mn0.60–0.80

Checked against 3 published copies

Si0.15–0.30

Checked against 3 published copies

Ni1.65–2.00

Checked against 3 published copies

Cr0.70–0.90

Checked against 3 published copies

Mo0.20–0.30

Checked against 3 published copies

P0.035 max

Checked against 3 published copies

S0.04 max

Checked against 3 published copies

4340 steel mechanical properties

By condition. Typical values vary by mill and bar size; specified minimums are what the standard guarantees.

Hot rolled, annealed, typical

Tensile strength, typical
108 ksi · 745 MPa

Only two makers publish this: AZoM and Alro

Yield strength (0.2 %), typical
68 ksi · 470 MPa

Only two makers publish this: AZoM and Alro

Elongation in 2 in., typical
22 %

Only two makers publish this: AZoM and Alro

Hardness, HB
Not enough published data yet

Machinability ratings

Each as its publisher prints it, with the baseline it is measured against. Ratings on different baselines are not comparable, so none are averaged.

  • 50 % (AISI 1212 = 100, annealed and cold drawn): AZoM
Sources7