Reamer drill size

11/16" reamer: drill size before reaming

For a 11/16" reamer, drill 43/64 (0.6719") in steel and 21/32 (0.6563") in aluminum. That leaves 0.0156" in steel and 0.0313" in aluminum, on the diameter. Three reamer makers give 0.0118–0.0170" in steel, median 0.0138", and 0.0157–0.0206" in aluminum, median 0.0200". That is over the aluminum span: 17 mm (0.6693") leaves 0.0182". Drills cut oversize, so check the first hole.

A 11/16" reamer’s hole, face on: the 43/64 (0.6719") drilled hole inside the reamed size, and the ring between them, 0.0156" on the diameter, that the reamer takes off.reamer Ø 11/16"drill Ø 43/64 (0.6719")leaves 0.0156" on Ø
The 11/16" reamer’s hole in steel, face on: the drilled hole and the stock the reamer takes off. Not to scale; the stock drawn far thicker than true.

Drill and stock for a 11/16" reamer

Median of 3 makers

11/16" reamer: the makers' stock allowance, the drill and what it leaves, by material
MaterialStockDrillLeaves
SteelStock 0.0138", span 0.0118–0.0170"0.0138"Makers span 0.0118–0.0170"43/640.6719"0.0156"
AluminumStock 0.0200", span 0.0157–0.0206"0.0200"Makers span 0.0157–0.0206"21/320.6563"0.0313"Over the makers' span17 mm (0.6693") leaves 0.0182"

Stock is the makers' median, with their span, on the diameter. For an inch reamer, the drill is the largest fraction, number or letter drill at or under the reamer size minus the makers' median stock; for a metric reamer, the largest metric size Guhring stocks in its jobber drills. So it leaves at least the median. Leaves is the reamer size minus the drill, on the diameter. Where it leaves more than the top of the makers' span, the drill that lands inside it nearest the median is named under it, from either list: the fraction, number and letter drills or Guhring's metric sizes. Where none lands, it says so. Drills cut oversize, so check the first hole.

Sources

Steel is Redline's low carbon steels, Helion's steels up to 700 N/mm² and Super Tool's 2 %; aluminum is Redline's aluminum alloys, Helion's light alloys and Super Tool's 3 %. Super Tool's rule is for carbide reamers.