Surface finish chart
Ra in µm and µin with the ISO N grades, what finish each process usually leaves, and the symbols on a print. To figure the finish a feed and nose radius will leave, use the surface finish calculator.
Ra, N grades and RMS
The µin column is the value charts and prints use (125 for 3.2 µm); the exact conversion is 39.37 µin per µm. RMS (Rq) is about1.11 × Ra, exact only for a sine-shaped profile, so treat it as an estimate.
| N grade | Ra µm | Ra µin | Exact µin | RMS ≈ µin |
|---|---|---|---|---|
| N1 | 0.025 | 1 | 0.98 | 1.1 |
| N2 | 0.05 | 2 | 1.97 | 2.2 |
| N3 | 0.1 | 4 | 3.94 | 4.4 |
| N4 | 0.2 | 8 | 7.87 | 8.9 |
| N5 | 0.4 | 16 | 15.7 | 18 |
| N6 | 0.8 | 32 | 31.5 | 36 |
| N7 | 1.6 | 63 | 63.0 | 70 |
| N8 | 3.2 | 125 | 126.0 | 139 |
| N9 | 6.3 | 250 | 248.0 | 278 |
| N10 | 12.5 | 500 | 492.1 | 555 |
| N11 | 25 | 1000 | 984.3 | 1,111 |
| N12 | 50 | 2000 | 1,968.5 | 2,221 |
Two published copies agree
ISO 1302 was withdrawn in 2021 for ISO 21920-1, which drops the N grades, but many drawings still carry them. Rz is not converted here: there is no fixed ratio between Ra and Rz, and charts that print one disagree.
Ra by process
The ASME B46.1 chart: "typical" is the average application, "possible" includes less frequent application under special conditions. Real finish depends on the tool, feed, rigidity and material.
| Process | Typical Ra | Possible Ra |
|---|---|---|
| Flame cutting | 25–12.5 µm1000–500 µin | 50–6.3 µm2000–250 µin |
| Sawing | 25–1.6 µm1000–63 µin | 50–0.8 µm2000–32 µin |
| Planing, shaping | 12.5–1.6 µm500–63 µin | 25–0.4 µm1000–16 µin |
| Drilling | 6.3–1.6 µm250–63 µin | 12.5–0.8 µm500–32 µin |
| Milling | 6.3–0.8 µm250–32 µin | 25–0.2 µm1000–8 µin |
| Broaching | 3.2–0.8 µm125–32 µin | 6.3–0.4 µm250–16 µin |
| Reaming | 3.2–0.8 µm125–32 µin | 6.3–0.4 µm250–16 µin |
| Laser | 6.3–0.8 µm250–32 µin | 6.3–0.2 µm250–8 µin |
| Boring, turning | 6.3–0.4 µm250–16 µin | 25–0.025 µm1000–1 µin |
| Roller burnishing | 0.8–0.2 µm32–8 µinMachinery's Handbook0.4–0.2 µm16–8 µinASME B46.1-1995 Two charts disagree: Machinery's Handbook 0.8–0.2 µm, ASME B46.1-1995 0.4–0.2 µm | 3.2–0.05 µm125–2 µinMachinery's Handbook0.8–0.1 µm32–4 µinASME B46.1-1995 Two charts disagree: Machinery's Handbook 3.2–0.05 µm, ASME B46.1-1995 0.8–0.1 µm |
| Grinding | 1.6–0.1 µm63–4 µin | 6.3–0.025 µm250–1 µinMachinery's Handbook6.3–0.012 µm250–0.5 µinASME B46.1-1995 Two charts disagree: Machinery's Handbook 6.3–0.025 µm, ASME B46.1-1995 6.3–0.012 µm |
| Honing | 0.8–0.1 µm32–4 µin | 1.6–0.025 µm63–1 µin |
| Polishing | 0.4–0.1 µm16–4 µin | 0.8–0.012 µm32–0.5 µin |
| Lapping | 0.4–0.05 µm16–2 µin | 0.8–0.012 µm32–0.5 µin |
| Superfinishing | 0.2–0.025 µm8–1 µin | 0.8–0.012 µm32–0.5 µin |
Two published copies agree
Where the two copies differ (roller burnishing, and grinding's finest value) both are shown. Electrical discharge machining is left out: neither copy's bar can be read to a step.
Surface finish symbols
The Ra value is written above the symbol's long leg; the lay symbol goes beside it.
Basic symbol
Any process may produce the surface.
Bar across the V
Material must be removed by machining (turning, milling, grinding …), so leave stock for it.
Circle in the V
No material may be removed: leave the surface as cast, forged, rolled or molded.
Lay (direction of the tool marks)
- =
- Parallel to the plane of projection of the view the symbol is on
- ⊥
- Perpendicular to the plane of projection of the view the symbol is on
- X
- Crossed in two slant directions (a honed crosshatch)
- M
- Multidirectional
- C
- Approximately circular about the center of the surface (a faced part)
- R
- Approximately radial from the center of the surface
Two published copies agree
Newer editions (ASME Y14.36-2018, ISO 21920-1) add P for particulate or non-directional lay; only one of the copies read gives it, so it isn't listed yet.
Sources8
- IS 10719:1983 (ISO 1302-1978), Table 1: roughness values Ra and roughness grade numbers (archived Nov 16, 2026)
- RoyMech, Surface texture equivalents (archived May 16, 2026)
- Machinery's Handbook, 25th ed., p. 708: Surface roughness produced by common production methods (as reprinted by CAB Worldwide) (archived May 20, 2025)
- Bal Seal Engineering, TR-29 Methods of obtaining surface finishes, Figure 2 (source: ASME B46.1-1995) (archived Sep 1, 2024)
- IS 10719:1983, Method for indication of surface texture on technical drawings (the Indian adoption of ISO 1302) (archived Nov 16, 2026)
- Wevolver, Surface finish symbols: how to read a drawing callout (ASME Y14.36-2018, ISO 21920-1:2021)
- Math: Rq ÷ Ra = π ÷ (2√2) ≈ 1.11 for a sine-shaped profile (from the definitions of Ra and Rq in ISO 4287 / ASME B46.1)
- RoyMech: "There is no mathematical relationship between Ra and Rt" (why Rz is not converted here) (archived May 16, 2026)