ISO 286 · Shaft

c11 shaft tolerance

c11 tolerance on a 25 mm shaft is −0.110 / −0.240 mm, so the shaft measures 24.760–24.890 mm. A c shaft sits wholly below the nominal size, so it clears an H hole. Grade 11 (IT11) sets the band’s width; the chart below gives it for every size to 500 mm.

c11 shaft tolerance zone for every size range from 0–3 mm to 450–500 mm, against the zero line; 18–30 mm is −110 / −240 µm.tolerance zone c11, 18–30 mm: −110 / −240 µmsize range 0–3 to 450–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

c11 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3−60−120−0.00236−0.00472
3–6−70−145−0.00276−0.00571
6–10−80−170−0.00315−0.00669
10–18−95−205−0.00374−0.00807
18–30−110−240−0.00433−0.00945
30–40−120−280−0.00472−0.01102
40–50−130−290−0.00512−0.01142
50–65−140−330−0.00551−0.01299
65–80−150−340−0.00591−0.01339
80–100−170−390−0.00669−0.01535
100–120−180−400−0.00709−0.01575
120–140−200−450−0.00787−0.01772
140–160−210−460−0.00827−0.01811
160–180−230−480−0.00906−0.01890
180–200−240−530−0.00945−0.02087
200–225−260−550−0.01024−0.02165
225–250−280−570−0.01102−0.02244
250–280−300−620−0.01181−0.02441
280–315−330−650−0.01299−0.02559
315–355−360−720−0.01417−0.02835
355–400−400−760−0.01575−0.02992
400–450−440−840−0.01732−0.03307
450–500−480−880−0.01890−0.03465

Checked against 3 published copies

Fits that use c11

Fits that use c11
  • H11/c11 · Loose running: Wide clearance for rough parts, or where it may get dirty or hot
Any size and fit in the calculator

Sources

Sources3