ISO 286 · Hole

D10 hole tolerance

D10 tolerance on a 25 mm hole is +0.149 / +0.065 mm, so the hole measures 25.065–25.149 mm. A D hole sits wholly above the nominal size, so it clears an h shaft. Grade 10 (IT10) sets the band’s width; the chart below gives it for every size to 500 mm.

d10 shaft on 25 mm: −0.065 / −0.149 mm. d10 shaft tolerance

D10 hole tolerance zone for every size range from 0–3 mm to 400–500 mm, against the zero line; 18–30 mm is +149 / +65 µm.tolerance zone D10, 18–30 mm: +149 / +65 µmsize range 0–3 to 400–500 mm
One band per size range against the zero line. The marked band holds 25 mm. Deviations to scale; the size ranges are evenly spaced, not to scale.

Limits by size

Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.

D10 limits by nominal size
Size, mmUpper µmLower µmUpper inLower in
0–3+60+20+0.00236+0.00079
3–6+78+30+0.00307+0.00118
6–10+98+40+0.00386+0.00157
10–18+120+50+0.00472+0.00197
18–30+149+65+0.00587+0.00256
30–50+180+80+0.00709+0.00315
50–80+220+100+0.00866+0.00394
80–120+260+120+0.01024+0.00472
120–180+305+145+0.01201+0.00571
180–250+355+170+0.01398+0.00669
250–315+400+190+0.01575+0.00748
315–400+440+210+0.01732+0.00827
400–500+480+230+0.01890+0.00906

Two published copies agree

Any size and fit in the calculator

Sources

Sources2