ISO 286 · Hole
E6 hole tolerance
E6 tolerance on a 25 mm hole is +0.053 / +0.040 mm, so the hole measures 25.040–25.053 mm. An E hole sits wholly above the nominal size, so it clears an h shaft. Grade 6 (IT6) sets the band’s width; the chart below gives it for every size to 500 mm.
e6 shaft on 25 mm: −0.040 / −0.053 mm. e6 shaft tolerance
Limits by size
Deviations from the nominal size, over the first size up to and including the second. Inches are µm ÷ 25,400; ANSI B4.2 inch tables round differently, by a tenth or so.
| Size, mm | Upper µm | Lower µm | Upper in | Lower in |
|---|---|---|---|---|
| 0–3 | +20 | +14 | +0.00079 | +0.00055 |
| 3–6 | +28 | +20 | +0.00110 | +0.00079 |
| 6–10 | +34 | +25 | +0.00134 | +0.00098 |
| 10–18 | +43 | +32 | +0.00169 | +0.00126 |
| 18–30 | +53 | +40 | +0.00209 | +0.00157 |
| 30–50 | +66 | +50 | +0.00260 | +0.00197 |
| 50–80 | +79 | +60 | +0.00311 | +0.00236 |
| 80–120 | +94 | +72 | +0.00370 | +0.00283 |
| 120–180 | +110 | +85 | +0.00433 | +0.00335 |
| 180–250 | +129 | +100 | +0.00508 | +0.00394 |
| 250–315 | +142 | +110 | +0.00559 | +0.00433 |
| 315–400 | +161 | +125 | +0.00634 | +0.00492 |
| 400–500 | +175 | +135 | +0.00689 | +0.00531 |
Checked against 3 published copies
Sources
Sources3
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables: