ISO 286 · Shaft · 180–250 mm

e8 shaft tolerance, 180–250 mm

e8 tolerance for shafts over 180 up to 250 mm is −0.100 / −0.172 mm (−0.00394 / −0.00677 in). A 200 mm e8 shaft measures 199.828–199.900 mm; a 250 mm one, 249.828–249.900 mm. The table gives each common size in the range in mm and inches.

e8 shaft tolerance zone, 180–250 mm: es −100 µm, ei −172 µm against the zero line.es −100 µmei −172 µmtolerance zone e8zero line 180–250 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

e8 limits, over 180 up to 250 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

e8 deviations over 180 up to 250 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
180–250−100−172−0.100−0.172−0.00394−0.0067772

Checked against 4 published copies

Common sizes, e8 shaft

The smallest and largest shaft each size allows. 180 mm itself belongs to the range below.

e8 smallest and largest size for common sizes over 180 up to 250 mm
SizeMin mmMax mmSize inMin inMax in
200 e8199.828199.9007.87407.867247.87008
220 e8219.828219.9008.66148.654658.65748
250 e8249.828249.9009.84259.835759.83858

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4