ISO 286 · Shaft · 315–400 mm
e8 shaft tolerance, 315–400 mm
e8 tolerance for shafts over 315 up to 400 mm is −0.125 / −0.214 mm (−0.00492 / −0.00843 in). A 400 mm e8 shaft measures 399.786–399.875 mm; a 350 mm one, 349.786–349.875 mm. The table gives each common size in the range in mm and inches.
e8 limits, over 315 up to 400 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 315–400 | −125 | −214 | −0.125 | −0.214 | −0.00492 | −0.00843 | 89 |
Checked against 4 published copies
Common sizes, e8 shaft
The smallest and largest shaft each size allows. 315 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 320 e8 | 319.786 | 319.875 | 12.5984 | 12.59000 | 12.59350 |
| 350 e8 | 349.786 | 349.875 | 13.7795 | 13.77110 | 13.77461 |
| 400 e8 | 399.786 | 399.875 | 15.7480 | 15.73961 | 15.74311 |
Checked against 4 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the e8 chart, checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)