ISO 286 · Shaft · 3–6 mm

f6 shaft tolerance, 3–6 mm

f6 tolerance for shafts over 3 up to 6 mm is −0.010 / −0.018 mm (−0.00039 / −0.00071 in). A 6 mm f6 shaft measures 5.982–5.990 mm; a 5 mm one, 4.982–4.990 mm. The table gives each common size in the range in mm and inches.

f6 shaft tolerance zone, 3–6 mm: es −10 µm, ei −18 µm against the zero line.es −10 µmei −18 µmtolerance zone f6zero line 3–6 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

f6 limits, over 3 up to 6 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

f6 deviations over 3 up to 6 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
3–6−10−18−0.010−0.018−0.00039−0.000718

Checked against 4 published copies

Common sizes, f6 shaft

The smallest and largest shaft each size allows. 3 mm itself belongs to the range below.

f6 smallest and largest size for common sizes over 3 up to 6 mm
SizeMin mmMax mmSize inMin inMax in
4 f63.9823.9900.15750.156770.15709
5 f64.9824.9900.19690.196140.19646
6 f65.9825.9900.23620.235510.23583

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4