ISO 286 · Shaft · 80–120 mm

f7 shaft tolerance, 80–120 mm

f7 tolerance for shafts over 80 up to 120 mm is −0.036 / −0.071 mm (−0.00142 / −0.00280 in). A 100 mm f7 shaft measures 99.929–99.964 mm; a 120 mm one, 119.929–119.964 mm. The table gives each common size in the range in mm and inches.

f7 shaft tolerance zone, 80–120 mm: es −36 µm, ei −71 µm against the zero line.es −36 µmei −71 µmtolerance zone f7zero line 80–120 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

f7 limits, over 80 up to 120 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

f7 deviations over 80 up to 120 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
80–120−36−71−0.036−0.071−0.00142−0.0028035

Checked against 4 published copies

Common sizes, f7 shaft

The smallest and largest shaft each size allows. 80 mm itself belongs to the range below.

f7 smallest and largest size for common sizes over 80 up to 120 mm
SizeMin mmMax mmSize inMin inMax in
90 f789.92989.9643.54333.540513.54189
100 f799.92999.9643.93703.934213.93559
110 f7109.929109.9644.33074.327914.32929
120 f7119.929119.9644.72444.721614.72299

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4