ISO 286 · Shaft · 3–6 mm

f8 shaft tolerance, 3–6 mm

f8 tolerance for shafts over 3 up to 6 mm is −0.010 / −0.028 mm (−0.00039 / −0.00110 in). A 6 mm f8 shaft measures 5.972–5.990 mm; a 5 mm one, 4.972–4.990 mm. The table gives each common size in the range in mm and inches.

f8 shaft tolerance zone, 3–6 mm: es −10 µm, ei −28 µm against the zero line.es −10 µmei −28 µmtolerance zone f8zero line 3–6 mm
The tolerance zone against the zero line (the basic size). es and ei are the shaft’s upper and lower deviations. Deviations to scale; the part itself is not drawn.

f8 limits, over 3 up to 6 mm

Deviations from the nominal size. Inches are the µm values ÷ 25,400.

f8 deviations over 3 up to 6 mm
Size, mmUpper µmLower µmUpper mmLower mmUpper inLower inBand µm
3–6−10−28−0.010−0.028−0.00039−0.0011018

Checked against 4 published copies

Common sizes, f8 shaft

The smallest and largest shaft each size allows. 3 mm itself belongs to the range below.

f8 smallest and largest size for common sizes over 3 up to 6 mm
SizeMin mmMax mmSize inMin inMax in
4 f83.9723.9900.15750.156380.15709
5 f84.9724.9900.19690.195750.19646
6 f85.9725.9900.23620.235120.23583

Checked against 4 published copies

ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.

Sources

Sources4