ISO 286 · Shaft · 315–400 mm
h11 shaft tolerance, 315–400 mm
h11 tolerance for shafts over 315 up to 400 mm is 0 / −0.360 mm (0 / −0.01417 in). A 400 mm h11 shaft measures 399.640–400.000 mm; a 350 mm one, 349.640–350.000 mm. The table gives each common size in the range in mm and inches.
h11 limits, over 315 up to 400 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 315–400 | 0 | −360 | 0 | −0.360 | 0 | −0.01417 | 360 |
Checked against 3 published copies
Common sizes, h11 shaft
The smallest and largest shaft each size allows. 315 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 320 h11 | 319.640 | 320.000 | 12.5984 | 12.58425 | 12.59843 |
| 350 h11 | 349.640 | 350.000 | 13.7795 | 13.76535 | 13.77953 |
| 400 h11 | 399.640 | 400.000 | 15.7480 | 15.73386 | 15.74803 |
Checked against 3 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources3
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the h11 chart, checked against these published copies of the tables: