ISO 286 · Shaft · 80–120 mm
h11 shaft tolerance, 80–120 mm
h11 tolerance for shafts over 80 up to 120 mm is 0 / −0.220 mm (0 / −0.00866 in). A 100 mm h11 shaft measures 99.780–100.000 mm; a 120 mm one, 119.780–120.000 mm. The table gives each common size in the range in mm and inches.
h11 limits, over 80 up to 120 mm
Deviations from the nominal size. Inches are the µm values ÷ 25,400.
| Size, mm | Upper µm | Lower µm | Upper mm | Lower mm | Upper in | Lower in | Band µm |
|---|---|---|---|---|---|---|---|
| 80–120 | 0 | −220 | 0 | −0.220 | 0 | −0.00866 | 220 |
Checked against 3 published copies
Common sizes, h11 shaft
The smallest and largest shaft each size allows. 80 mm itself belongs to the range below.
| Size | Min mm | Max mm | Size in | Min in | Max in |
|---|---|---|---|---|---|
| 90 h11 | 89.780 | 90.000 | 3.5433 | 3.53465 | 3.54331 |
| 100 h11 | 99.780 | 100.000 | 3.9370 | 3.92835 | 3.93701 |
| 110 h11 | 109.780 | 110.000 | 4.3307 | 4.32205 | 4.33071 |
| 120 h11 | 119.780 | 120.000 | 4.7244 | 4.71575 | 4.72441 |
Checked against 3 published copies
ISO fits are metric; the inch columns convert them. ANSI B4.2 inch tables round differently, by a tenth or so.
Sources
Sources3
ISO 286-1 and 286-2. Every limit on this page comes from the same engine as the h11 chart, checked against these published copies of the tables: